Replication Technique
2 cases · 6 images
Crevice Corrosion in a Subsea System — Aspect Before Analysis
Replication Technique — sub-branches

ML00161 / Mar.2020
Brittle Fracture of a High Strength Socket
M - Medium Carbon Tool SteelP - ToolAp - Oil and GasCd - Brittle Fracture
Cm - As polishedDf - Brittle Cracks

ML00092 / Sep.2017
MIC of a Valve Body
M - Martensitic Stainless SteelP - Valve BodyAp - Oil and GasCd - Brittle Behavior
Cm - As polishedDf - Microcracks
More from these cases

ML00092 / Sep.2017
MIC of a Valve Body
M - Martensitic Stainless SteelP - Valve BodyAp - Oil and GasCd - Brittle Behavior
Cm - Kalling etched, OMDf - Martensite

ML00092 / Sep.2017
MIC of a Valve Body
M - Martensitic Stainless SteelP - Valve BodyAp - Oil and GasCd - Brittle Behavior
Cm - Kalling etched, OMDf - Martensite

ML00092 / Sep.2017
MIC of a Valve Body
M - Martensitic Stainless SteelP - Valve BodyAp - Oil and GasCd - Brittle Behavior
Cm - Kalling etched, OMDf - Pitting

ML00092 / Sep.2017
MIC of a Valve Body
M - Martensitic Stainless SteelP - Valve BodyAp - Oil and GasCd - Brittle Behavior
Cm - Kalling etched, OMDf - Microcracks