Optical Microscope

6 cases · 19 images

Crevice Corrosion in a Subsea System — Aspect Before Analysis

Micrography of the longitudinal section, in the center of the thickness of the pin, presenting an aligned ferritic-austeinitic structure.
180
ML00146 / Jul.2018
Plastic Deformation of a SDSS Riser Pin
M - Super Duplex Stainless SteelP - PinAp - O&G Well DrillingCd - Bending
Cm - NaOH Electrolytic Etched MicroDf - Ferrite and Austenite
ML00135 / May.2018
MIC of a Non Magnetic Drilling Tool
M - High Mn Austenitic SteelP - Tubular ForgingAp - O&G Well DrillingCd - Pitting Corrosion
Cm - Oxalic Acid Electrolytic EtchDf - Austenite
ML00110 / Jan.2018
Non Conformance in Spray and Fuse Pin
M - Low Alloy Medium Carbon QTP - Tubular ForgingAp - O&G Well DrillingCd - Heat Treatment Defect
Cm - Nital Etched Micrography by OMDf - Ferrite and Pearlite
ML00109 / Jan.2018
Thermal Spray and Fuse Layer in Forged Pin
M - Low Alloy Medium Carbon QTP - Tubular ForgingAp - O&G Well DrillingCd - Thermal spray
Cm - Nital Etched Micrography by OMDf - Martensite
ML00100 / Nov.2017
Superduplex Tubing to Forging Welded Joint
M - Super Duplex Stainless SteelP - Fabrication WeldAp - SubseaCd - Welding
Cm - NaOH Electrolytic Etched MicroDf - Duplex structure
ML00082 / Dec.2017
Corrosion Fatigue of a Drilling Tool
M - Low Alloy Medium Carbon QTP - Tubular ForgingAp - O&G Well DrillingCd - Corrosion Fatigue
Cm - Nital Etched Micrography by OMDf - Martensite

More from these cases

ML00146 — Plastic Deformation of a SDSS Riser PinM - Super Duplex Stainless SteelP - PinAp - O&G Well DrillingCd - Bending
Micrography of a longitudinal section, at the surface of the pin, where the thermal spray layer is sound. The thickness of the layer is about 0.3 mm.
168
ML00146 / Jul.2018
Plastic Deformation of a SDSS Riser Pin
M - Super Duplex Stainless SteelP - PinAp - O&G Well DrillingCd - Bending
Cm - NaOH Electrolytic Etched MicroDf - Coating Layer
Micrographic detail of a longitudinal section of the pin, at the surface, evidencing the thermal spray layer, about 0.3 mm.  The layer presents typical characteristics of multiple layers, low amount of entrapped oxides and pores.  The interface presents a high roughness level for a good adherence and some entrapped oxides. The structure of the SDSS substrate did not show thermal effects.
154
ML00146 / Jul.2018
Plastic Deformation of a SDSS Riser Pin
M - Super Duplex Stainless SteelP - PinAp - O&G Well DrillingCd - Bending
Cm - NaOH Electrolytic Etched MicroDf - Coating Layer
ML00135 — MIC of a Non Magnetic Drilling ToolM - High Mn Austenitic SteelP - Tubular ForgingAp - O&G Well DrillingCd - Pitting Corrosion
ML00135 / May.2018
MIC of a Non Magnetic Drilling Tool
M - High Mn Austenitic SteelP - Tubular ForgingAp - O&G Well DrillingCd - Pitting Corrosion
Cm - Oxalic Acid Electrolytic EtchDf - Austenite
ML00110 — Non Conformance in Spray and Fuse PinM - Low Alloy Medium Carbon QTP - Tubular ForgingAp - O&G Well DrillingCd - Heat Treatment Defect
ML00110 / Jan.2018
Non Conformance in Spray and Fuse Pin
M - Low Alloy Medium Carbon QTP - Tubular ForgingAp - O&G Well DrillingCd - Heat Treatment Defect
Cm - Nital Etched Micrography by OMDf - Ferrite and Pearlite
ML00110 / Jan.2018
Non Conformance in Spray and Fuse Pin
M - Low Alloy Medium Carbon QTP - Tubular ForgingAp - O&G Well DrillingCd - Heat Treatment Defect
Cm - Nital Etched Micrography by OMDf - Ferrite and Pearlite
ML00109 — Thermal Spray and Fuse Layer in Forged PinM - Low Alloy Medium Carbon QTP - Tubular ForgingAp - O&G Well DrillingCd - Thermal spray
ML00109 / Jan.2018
Thermal Spray and Fuse Layer in Forged Pin
M - Low Alloy Medium Carbon QTP - Tubular ForgingAp - O&G Well DrillingCd - Thermal spray
Cm - Nital Etched Micrography by OMDf - Martensite
ML00109 / Jan.2018
Thermal Spray and Fuse Layer in Forged Pin
M - Low Alloy Medium Carbon QTP - Tubular ForgingAp - O&G Well DrillingCd - Thermal spray
Cm - Nital Etched Micrography by OMDf - Bainite
ML00109 / Jan.2018
Thermal Spray and Fuse Layer in Forged Pin
M - Low Alloy Medium Carbon QTP - Tubular ForgingAp - O&G Well DrillingCd - Thermal spray
Cm - Nital Etched Micrography by OMDf - Bainite
ML00100 — Superduplex Tubing to Forging Welded JointM - Super Duplex Stainless SteelP - Fabrication WeldAp - SubseaCd - Welding
ML00100 / Nov.2017
Superduplex Tubing to Forging Welded Joint
M - Super Duplex Stainless SteelP - Fabrication WeldAp - SubseaCd - Welding
Cm - NaOH Electrolytic Etched MicroDf - Duplex structure
ML00100 / Nov.2017
Superduplex Tubing to Forging Welded Joint
M - Super Duplex Stainless SteelP - Fabrication WeldAp - SubseaCd - Welding
Cm - NaOH Electrolytic Etched MicroDf - Duplex structure
ML00100 / Nov.2017
Superduplex Tubing to Forging Welded Joint
M - Super Duplex Stainless SteelP - Fabrication WeldAp - SubseaCd - Welding
Cm - NaOH Electrolytic Etched MicroDf - Coarse Structure
ML00082 — Corrosion Fatigue of a Drilling ToolM - Low Alloy Medium Carbon QTP - Tubular ForgingAp - O&G Well DrillingCd - Corrosion Fatigue
ML00082 / Dec.2017
Corrosion Fatigue of a Drilling Tool
M - Low Alloy Medium Carbon QTP - Tubular ForgingAp - O&G Well DrillingCd - Corrosion Fatigue
Cm - Nital Etched Micrography by OMDf - Banded Structure
ML00082 / Dec.2017
Corrosion Fatigue of a Drilling Tool
M - Low Alloy Medium Carbon QTP - Tubular ForgingAp - O&G Well DrillingCd - Corrosion Fatigue
Cm - Nital Etched Micrography by OMDf - Banded Structure