Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00151 / Dec.2018
Ferritic Stainless Steel of a Flatware Fork
M - Ferritic Stainless SteelP - Foodstuff ArticleAp - KitchenCd - Typical manufacturing
Cm - Micro by OM, HCl + Ethanol + Picric AcidDf - Plastic Deformation
ML00145 / Sep.2018
Impact of a .380 Winchester on 6061 T6 Plate
M - Aluminum Magnesium SiliconP - Rolled PlateAp - StructureCd - Pierced
Cm - Keller Etched Micrography by OMDf - Plastic Deformation
ML00135 / May.2018
MIC of a Non Magnetic Drilling Tool
M - High Mn Austenitic SteelP - Tubular ForgingAp - O&G Well DrillingCd - Pitting Corrosion
Cm - Oxalic Acid Electrolytic EtchDf - Localized Corrosion
ML00078 / Jun.2017
Hydrogen Cracking of IN 718 Subsea Connector
M - NiCrFe AlloyP - ForgingAp - SubseaCd - Hydrogen Embrittlement
Cm - Kalling Etched Micrography by OMDf - Fracture
ML00065 / May.2017
Erosion Corrosion of Monel Piping
M - NiCu AlloyP - Seamless PipeAp - Chemical IndustryCd - Erosion Corrosion
Cm - Kalling Etched Micrography by OMDf - Thinning
ML00059 / Feb.2018
Intergranular Corrosion of Aluminum Piping
M - Aluminum ManganeseP - Welded JointAp - Chemical IndustryCd - Intergranular Corrosion
Cm - Keller Etched Micrography by OMDf - Localized Corrosion
ML00041 / Jun.2017
Fatigue Fracture of Inconel 718 Spline Shaft
M - NiCrFe AlloyP - ShaftAp - Oil and GasCd - Vibration Induced Fatigue
Cm - Kalling Etched Micrography by OMDf - Transgranular Cracking
The pipe base metal, at the internal surface, presents a hydride layer showing that the environment is absorbing hydrogen.  Although there are microcracks in this layer it did not detach in the base metal.
102
ML00005 / Apr.2017
Environmental Hydrogen Damage in Ti Pipe
M - Unalloyed TitaniumP - Longitudinal Seam Welded PipeAp - PipingCd - Hydride Formation
Cm - Kroll Etched Micrography by OMDf - Hydride Formation

More from these cases

ML00151 — Ferritic Stainless Steel of a Flatware ForkM - Ferritic Stainless SteelP - Foodstuff ArticleAp - KitchenCd - Typical manufacturing
ML00151 / Dec.2018
Ferritic Stainless Steel of a Flatware Fork
M - Ferritic Stainless SteelP - Foodstuff ArticleAp - KitchenCd - Typical manufacturing
Cm - Micro by OM, HCl + Ethanol + Picric AcidDf - Plastic Deformation
ML00145 — Impact of a .380 Winchester on 6061 T6 PlateM - Aluminum Magnesium SiliconP - Rolled PlateAp - StructureCd - Pierced
ML00145 / Sep.2018
Impact of a .380 Winchester on 6061 T6 Plate
M - Aluminum Magnesium SiliconP - Rolled PlateAp - StructureCd - Pierced
Cm - Keller Etched Micrography by OMDf - Plastic Deformation
ML00145 / Sep.2018
Impact of a .380 Winchester on 6061 T6 Plate
M - Aluminum Magnesium SiliconP - Rolled PlateAp - StructureCd - Pierced
Cm - Keller Etched Micrography by OMDf - Plastic Deformation
ML00145 / Sep.2018
Impact of a .380 Winchester on 6061 T6 Plate
M - Aluminum Magnesium SiliconP - Rolled PlateAp - StructureCd - Pierced
Cm - Keller Etched Micrography by OMDf - Ductile Fracture
ML00145 / Sep.2018
Impact of a .380 Winchester on 6061 T6 Plate
M - Aluminum Magnesium SiliconP - Rolled PlateAp - StructureCd - Pierced
Cm - Keller Etched Micrography by OMDf - Ductile Crack
ML00145 / Sep.2018
Impact of a .380 Winchester on 6061 T6 Plate
M - Aluminum Magnesium SiliconP - Rolled PlateAp - StructureCd - Pierced
Cm - Keller Etched Micrography by OMDf - Plastic Deformation

+5 more from this case →

ML00135 — MIC of a Non Magnetic Drilling ToolM - High Mn Austenitic SteelP - Tubular ForgingAp - O&G Well DrillingCd - Pitting Corrosion
ML00135 / May.2018
MIC of a Non Magnetic Drilling Tool
M - High Mn Austenitic SteelP - Tubular ForgingAp - O&G Well DrillingCd - Pitting Corrosion
Cm - Oxalic Acid Electrolytic EtchDf - Localized Corrosion
ML00078 — Hydrogen Cracking of IN 718 Subsea ConnectorM - NiCrFe AlloyP - ForgingAp - SubseaCd - Hydrogen Embrittlement
ML00078 / Jun.2017
Hydrogen Cracking of IN 718 Subsea Connector
M - NiCrFe AlloyP - ForgingAp - SubseaCd - Hydrogen Embrittlement
Cm - Kalling Etched Micrography by OMDf - Secondary Cracks
ML00078 / Jun.2017
Hydrogen Cracking of IN 718 Subsea Connector
M - NiCrFe AlloyP - ForgingAp - SubseaCd - Hydrogen Embrittlement
Cm - Kalling Etched Micrography by OMDf - Intergranular Cracking
ML00078 / Jun.2017
Hydrogen Cracking of IN 718 Subsea Connector
M - NiCrFe AlloyP - ForgingAp - SubseaCd - Hydrogen Embrittlement
Cm - Kalling Etched Micrography by OMDf - Secondary Cracks
ML00059 — Intergranular Corrosion of Aluminum PipingM - Aluminum ManganeseP - Welded JointAp - Chemical IndustryCd - Intergranular Corrosion
ML00059 / Feb.2018
Intergranular Corrosion of Aluminum Piping
M - Aluminum ManganeseP - Welded JointAp - Chemical IndustryCd - Intergranular Corrosion
Cm - Keller Etched Micrography by OMDf - Localized Corrosion
ML00059 / Feb.2018
Intergranular Corrosion of Aluminum Piping
M - Aluminum ManganeseP - Welded JointAp - Chemical IndustryCd - Intergranular Corrosion
Cm - Keller Etched Micrography by OMDf - Localized Corrosion
ML00041 — Fatigue Fracture of Inconel 718 Spline ShaftM - NiCrFe AlloyP - ShaftAp - Oil and GasCd - Vibration Induced Fatigue
ML00041 / Jun.2017
Fatigue Fracture of Inconel 718 Spline Shaft
M - NiCrFe AlloyP - ShaftAp - Oil and GasCd - Vibration Induced Fatigue
Cm - Kalling Etched Micrography by OMDf - Transgranular Crack
ML00005 — Environmental Hydrogen Damage in Ti PipeM - Unalloyed TitaniumP - Longitudinal Seam Welded PipeAp - PipingCd - Hydride Formation
ML00005 / Apr.2017
Environmental Hydrogen Damage in Ti Pipe
M - Unalloyed TitaniumP - Longitudinal Seam Welded PipeAp - PipingCd - Hydride Formation
Cm - Kroll Etched Micrography by OMDf - Localized Thinning
ML00005 / Apr.2017
Environmental Hydrogen Damage in Ti Pipe
M - Unalloyed TitaniumP - Longitudinal Seam Welded PipeAp - PipingCd - Hydride Formation
Cm - Micrography by OMDf - Brittle Cracks
ML00005 / Apr.2017
Environmental Hydrogen Damage in Ti Pipe
M - Unalloyed TitaniumP - Longitudinal Seam Welded PipeAp - PipingCd - Hydride Formation
Cm - Kroll Etched Micrography by OMDf - Localized Thinning