Optical Microscope
7 cases · 19 images
Crevice Corrosion in a Subsea System — Aspect Before Analysis
Optical Microscope — sub-branches

ML00167 / Aug.2020
Fatigue of a Flared Tubing Connection
M - Austenitic Stainless SteelP - TubingAp - EngineCd - Mechanical Fatigue
Cm - Oxalic Acid Electrolytic EtchDf - Plastic Deformation

ML00148 / Sep.2018
Brittle Fracture of a 420 SS Barrel Nut
M - Martensitic Stainless SteelP - Barrel NutAp - LiftingCd - Heat Treatment Defect
Cm - Kalling Etched Micrography by OMDf - Plastic Deformation

ML00145 / Sep.2018
Impact of a .380 Winchester on 6061 T6 Plate
M - Aluminum Magnesium SiliconP - Rolled PlateAp - StructureCd - Pierced
Cm - Keller Etched Micrography by OMDf - Plastic Deformation

ML00144 / Aug.2018
Impact of a .380 Winchester on Ti64 Plate
M - Ti6Al4VP - Rolled PlateAp - StructureCd - Non-Pierced
Cm - Micrography by OMDf - Plastic Deformation

ML00139 / Jun.2018
Hydrogen Fracture of a 17-4 PH Allen Bolt
M - Precipitation Hardened Stainless SteelP - Allen BoltAp - SubseaCd - Hydrogen Embrittlement
Cm - Kalling Etched Micrography by OMDf - Plastic Deformation

ML00007 / Dec.2020
Free Machining Brass in Shear Pin
M - BrassP - Machined PartAp - LiftingCd - Shear
Cm - FeCl3+HCl+H2O Etched MicroDf - Plastic Deformation

ML00027 / Apr.2017
Adhesive Wear of Spur Gear Rack
M - Medium Carbon SteelP - Spur GearAp - Mechanical IndustryCd - Adhesive Wear
Cm - Nital Etched Micrography by OMDf - Plastic Deformation
More from these cases

ML00148 / Sep.2018
Brittle Fracture of a 420 SS Barrel Nut
M - Martensitic Stainless SteelP - Barrel NutAp - LiftingCd - Heat Treatment Defect
Cm - Kalling Etched Micrography by OMDf - Plastic Deformation

ML00145 / Sep.2018
Impact of a .380 Winchester on 6061 T6 Plate
M - Aluminum Magnesium SiliconP - Rolled PlateAp - StructureCd - Pierced
Cm - Keller Etched Micrography by OMDf - Plastic Deformation

ML00145 / Sep.2018
Impact of a .380 Winchester on 6061 T6 Plate
M - Aluminum Magnesium SiliconP - Rolled PlateAp - StructureCd - Pierced
Cm - Keller Etched Micrography by OMDf - Plastic Deformation

ML00145 / Sep.2018
Impact of a .380 Winchester on 6061 T6 Plate
M - Aluminum Magnesium SiliconP - Rolled PlateAp - StructureCd - Pierced
Cm - Keller Etched Micrography by OMDf - Plastic Deformation

ML00145 / Sep.2018
Impact of a .380 Winchester on 6061 T6 Plate
M - Aluminum Magnesium SiliconP - Rolled PlateAp - StructureCd - Pierced
Cm - Keller Etched Micrography by OMDf - Plastic Deformation

ML00145 / Sep.2018
Impact of a .380 Winchester on 6061 T6 Plate
M - Aluminum Magnesium SiliconP - Rolled PlateAp - StructureCd - Pierced
Cm - Keller Etched Micrography by OMDf - Plastic Deformation

ML00027 / Apr.2017
Adhesive Wear of Spur Gear Rack
M - Medium Carbon SteelP - Spur GearAp - Mechanical IndustryCd - Adhesive Wear
Cm - Nital Etched Micrography by OMDf - Plastic Deformation

ML00027 / Apr.2017
Adhesive Wear of Spur Gear Rack
M - Medium Carbon SteelP - Spur GearAp - Mechanical IndustryCd - Adhesive Wear
Cm - Nital Etched Micrography by OMDf - Plastic Deformation

ML00027 / Apr.2017
Adhesive Wear of Spur Gear Rack
M - Medium Carbon SteelP - Spur GearAp - Mechanical IndustryCd - Adhesive Wear
Cm - Nital Etched Micrography by OMDf - Plastic Deformation

ML00027 / Apr.2017
Adhesive Wear of Spur Gear Rack
M - Medium Carbon SteelP - Spur GearAp - Mechanical IndustryCd - Adhesive Wear
Cm - Nital Etched Micrography by OMDf - Plastic Deformation

ML00027 / Apr.2017
Adhesive Wear of Spur Gear Rack
M - Medium Carbon SteelP - Spur GearAp - Mechanical IndustryCd - Adhesive Wear
Cm - Nital Etched Micrography by OMDf - Plastic Deformation