Optical Microscope

27 cases · 239 images

Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00053 / Mar.2017
SAW Longitudinal Seam of X70 Pipe
M - Microalloyed SteelP - Longitudinal Seam Welded PipeAp - SubseaCd - Welding
Cm - Nital Etched Micrography by OMDf - Base Metal
The plate longitudinal section presents a granular refined structure. Biphasic.
340
ML00029 / Jan.2017
Titanium Plate for Subsea Application
M - Ti6Al4VP - Rolled PlateAp - StructureCd - Typical manufacturing
Cm - Micrography by OM, HF + HNO3 + H2O etchDf - Grain refined structure
The bar presented a large prior beta grain size and acicular alpha. Biphasic structure.
420
ML00028 / Jan.2017
Titanium Bar for Subsea Application
M - Ti6Al4VP - BarAp - StructureCd - Typical manufacturing
Cm - Micrography by OM, HF + HNO3 + H2O etchDf - Coarse Structure

More from these cases

ML00053 — SAW Longitudinal Seam of X70 PipeM - Microalloyed SteelP - Longitudinal Seam Welded PipeAp - SubseaCd - Welding
ML00053 / Mar.2017
SAW Longitudinal Seam of X70 Pipe
M - Microalloyed SteelP - Longitudinal Seam Welded PipeAp - SubseaCd - Welding
Cm - Nital Etched Micrography by OMDf - Base Metal
ML00053 / Mar.2017
SAW Longitudinal Seam of X70 Pipe
M - Microalloyed SteelP - Longitudinal Seam Welded PipeAp - SubseaCd - Welding
Cm - Nital Etched Micrography by OMDf - Base Metal
ML00053 / Mar.2017
SAW Longitudinal Seam of X70 Pipe
M - Microalloyed SteelP - Longitudinal Seam Welded PipeAp - SubseaCd - Welding
Cm - Nital Etched Micrography by OMDf - Fusion Line
ML00053 / Mar.2017
SAW Longitudinal Seam of X70 Pipe
M - Microalloyed SteelP - Longitudinal Seam Welded PipeAp - SubseaCd - Welding
Cm - Nital Etched Micrography by OMDf - Weld Metal
ML00053 / Mar.2017
SAW Longitudinal Seam of X70 Pipe
M - Microalloyed SteelP - Longitudinal Seam Welded PipeAp - SubseaCd - Welding
Cm - Nital Etched Micrography by OMDf - Fusion Line

+6 more from this case →

ML00029 — Titanium Plate for Subsea ApplicationM - Ti6Al4VP - Rolled PlateAp - StructureCd - Typical manufacturing
ML00029 / Jan.2017
Titanium Plate for Subsea Application
M - Ti6Al4VP - Rolled PlateAp - StructureCd - Typical manufacturing
Cm - Micrography by OM, HF + HNO3 + H2O etchDf - Two phases
ML00029 / Jan.2017
Titanium Plate for Subsea Application
M - Ti6Al4VP - Rolled PlateAp - StructureCd - Typical manufacturing
Cm - Micrography by OM, HF + HNO3 + H2O etchDf - Two phases
ML00028 — Titanium Bar for Subsea ApplicationM - Ti6Al4VP - BarAp - StructureCd - Typical manufacturing
ML00028 / Jan.2017
Titanium Bar for Subsea Application
M - Ti6Al4VP - BarAp - StructureCd - Typical manufacturing
Cm - Micrography by OM, HF + HNO3 + H2O etchDf - Two phases
Acicular alpha structure in a biphasic alloy of a large prior beta grain size.  4" diameter bar.
100
ML00028 / Jan.2017
Titanium Bar for Subsea Application
M - Ti6Al4VP - BarAp - StructureCd - Typical manufacturing
Cm - Micrography by OM, HF + HNO3 + H2O etchDf - Acicular Alpha