Optical Microscope
3 cases · 60 images
Crevice Corrosion in a Subsea System — Aspect Before Analysis
Optical Microscope — sub-branches

ML00155 / Jan.2020
Failure of a Prestressed Concrete Steel Strand
M - High Carbon SteelP - Wire RopeAp - StructureCd - Corrosion Fatigue
Cm - Nital Etched Micrography by OMDf - Longitudinal Section

ML00145 / Sep.2018
Impact of a .380 Winchester on 6061 T6 Plate
M - Aluminum Magnesium SiliconP - Rolled PlateAp - StructureCd - Pierced
Cm - Keller Etched Micrography by OMDf - Aligned particles

ML00143 / Aug.2018
Impact of a .308 Winchester on A36 Plate
M - Low Carbon SteelP - Rolled PlateAp - StructureCd - Pierced
Cm - Nital Etched Micrography by OMDf - Ferrite and Pearlite
More from these cases

ML00155 / Jan.2020
Failure of a Prestressed Concrete Steel Strand
M - High Carbon SteelP - Wire RopeAp - StructureCd - Corrosion Fatigue
Cm - Nital Etched Micrography by OMDf - Predominantly Pearlitic

ML00155 / Jan.2020
Failure of a Prestressed Concrete Steel Strand
M - High Carbon SteelP - Wire RopeAp - StructureCd - Corrosion Fatigue
Cm - Nital Etched Micrography by OMDf - Corrosion

ML00155 / Jan.2020
Failure of a Prestressed Concrete Steel Strand
M - High Carbon SteelP - Wire RopeAp - StructureCd - Corrosion Fatigue
Cm - Nital Etched Micrography by OMDf - Cracks

ML00155 / Jan.2020
Failure of a Prestressed Concrete Steel Strand
M - High Carbon SteelP - Wire RopeAp - StructureCd - Corrosion Fatigue
Cm - Nital Etched Micrography by OMDf - Ductile Fracture

ML00155 / Jan.2020
Failure of a Prestressed Concrete Steel Strand
M - High Carbon SteelP - Wire RopeAp - StructureCd - Corrosion Fatigue
Cm - As polished micrographyDf - Ductile Fracture

ML00145 / Sep.2018
Impact of a .380 Winchester on 6061 T6 Plate
M - Aluminum Magnesium SiliconP - Rolled PlateAp - StructureCd - Pierced
Cm - Keller Etched Micrography by OMDf - Aligned particles

ML00145 / Sep.2018
Impact of a .380 Winchester on 6061 T6 Plate
M - Aluminum Magnesium SiliconP - Rolled PlateAp - StructureCd - Pierced
Cm - Keller Etched Micrography by OMDf - Granular structure

ML00145 / Sep.2018
Impact of a .380 Winchester on 6061 T6 Plate
M - Aluminum Magnesium SiliconP - Rolled PlateAp - StructureCd - Pierced
Cm - Keller Etched Micrography by OMDf - Granular structure

ML00145 / Sep.2018
Impact of a .380 Winchester on 6061 T6 Plate
M - Aluminum Magnesium SiliconP - Rolled PlateAp - StructureCd - Pierced
Cm - Keller Etched Micrography by OMDf - Strain Hardened

ML00145 / Sep.2018
Impact of a .380 Winchester on 6061 T6 Plate
M - Aluminum Magnesium SiliconP - Rolled PlateAp - StructureCd - Pierced
Cm - Keller Etched Micrography by OMDf - Plastic Deformation

ML00143 / Aug.2018
Impact of a .308 Winchester on A36 Plate
M - Low Carbon SteelP - Rolled PlateAp - StructureCd - Pierced
Cm - Nital Etched Micrography by OMDf - Ferrite and Pearlite

ML00143 / Aug.2018
Impact of a .308 Winchester on A36 Plate
M - Low Carbon SteelP - Rolled PlateAp - StructureCd - Pierced
Cm - Nital Etched Micrography by OMDf - Ferrite and Pearlite

ML00143 / Aug.2018
Impact of a .308 Winchester on A36 Plate
M - Low Carbon SteelP - Rolled PlateAp - StructureCd - Pierced
Cm - Nital Etched Micrography by OMDf - Ferrite and Pearlite

ML00143 / Aug.2018
Impact of a .308 Winchester on A36 Plate
M - Low Carbon SteelP - Rolled PlateAp - StructureCd - Pierced
Cm - As polished micrographyDf - Transverse Section

ML00143 / Aug.2018
Impact of a .308 Winchester on A36 Plate
M - Low Carbon SteelP - Rolled PlateAp - StructureCd - Pierced
Cm - As polished micrographyDf - Melted film