Optical Microscope

3 cases · 49 images for “fatigue”

Crevice Corrosion in a Subsea System — Aspect Before Analysis

The tube microstructure is ferritic-pearlitic, typical of this kind of material.  No evidences of microstrutural changes were detected (no overheating, no decarburization).
177
ML00163 / Jun.2020
Corrosion Fatigue of a Boiler Waterwall Tube
M - Low Carbon SteelP - Seamless tubeAp - BoilerCd - Corrosion Fatigue
Cm - Nital Etched Micrography by OMDf - Ferrite and Pearlite
Micrography of the plate in a longitudinal section, presenting a typical ferritic pearlitic structure, banded.  The plate is 22 mm thick.
182
ML00119 / Feb.2018
Thermal Fatigue of a Marine Boiler
M - Low Carbon SteelP - Fabrication WeldAp - ShipCd - Thermal Fatigue
Cm - Nital Etched Micrography by OMDf - Banded Structure
The micrography of the longitudinal section of the tube, close to OD, shows the paralel cracks, filled with oxides, perpendicular to the surface.
1441
ML00104 / Dec.2017
Thermal Fatigue of a Boiler Tube
M - Low Carbon SteelP - Autogenously Welded TubeAp - BoilerCd - Thermal Fatigue
Cm - As polished micrographyDf - Close to the External Surface

More from these cases

ML00163 — Corrosion Fatigue of a Boiler Waterwall TubeM - Low Carbon SteelP - Seamless tubeAp - BoilerCd - Corrosion Fatigue
The internal side of the tube presented multiple cracks, filled with oxides, blunt-tipped, typical of a corrosion fatigue cracking mechanism.
160
ML00163 / Jun.2020
Corrosion Fatigue of a Boiler Waterwall Tube
M - Low Carbon SteelP - Seamless tubeAp - BoilerCd - Corrosion Fatigue
Cm - As polished micrographyDf - Parallel cracks
Micrographic detail of the corrosion cracking from internal side of the tube, in several points at the tube surface.
156
ML00163 / Jun.2020
Corrosion Fatigue of a Boiler Waterwall Tube
M - Low Carbon SteelP - Seamless tubeAp - BoilerCd - Corrosion Fatigue
Cm - As polished micrographyDf - Corrosion Cracking
Low magnification micrography of the multiple cracks, parallel, transgranular. No evidences of microstrutural changes (heat evolution or decarburization).
127
ML00163 / Jun.2020
Corrosion Fatigue of a Boiler Waterwall Tube
M - Low Carbon SteelP - Seamless tubeAp - BoilerCd - Corrosion Fatigue
Cm - Nital Etched Micrography by OMDf - Transgranular Cracking
Micrography presenting the internal tube surface with several parallel cracks, some still in the beginning (less than 0.1 mm deep).
115
ML00163 / Jun.2020
Corrosion Fatigue of a Boiler Waterwall Tube
M - Low Carbon SteelP - Seamless tubeAp - BoilerCd - Corrosion Fatigue
Cm - Nital Etched Micrography by OMDf - Parallel cracks
Micrography of the crack tip, initiated from the internal tube surface.  The crack is transgranular, filled with oxides and blunt-tipped.
109
ML00163 / Jun.2020
Corrosion Fatigue of a Boiler Waterwall Tube
M - Low Carbon SteelP - Seamless tubeAp - BoilerCd - Corrosion Fatigue
Cm - Nital Etched Micrography by OMDf - Transgranular Cracking

+9 more from this case →

ML00119 — Thermal Fatigue of a Marine BoilerM - Low Carbon SteelP - Fabrication WeldAp - ShipCd - Thermal Fatigue
Micrography of the plate in a longitudinal section, presenting a typical ferritic pearlitic structure, banded.
165
ML00119 / Feb.2018
Thermal Fatigue of a Marine Boiler
M - Low Carbon SteelP - Fabrication WeldAp - ShipCd - Thermal Fatigue
Cm - Nital Etched Micrography by OMDf - Ferrite and Pearlite
Micrographic detail of the ferritic pearlitic structure of the plate in the longitudinal section.
147
ML00119 / Feb.2018
Thermal Fatigue of a Marine Boiler
M - Low Carbon SteelP - Fabrication WeldAp - ShipCd - Thermal Fatigue
Cm - Nital Etched Micrography by OMDf - Ferrite and Pearlite
Micrography of the weld metal in the center os the weld. Columnar grains (of the previous austenite) with primary ferrite in the grain boundaries; ferrite with aligned second phases and acicular ferrite, intragranular.
137
ML00119 / Feb.2018
Thermal Fatigue of a Marine Boiler
M - Low Carbon SteelP - Fabrication WeldAp - ShipCd - Thermal Fatigue
Cm - Nital Etched Micrography by OMDf - Weld Metal
Micrography of the weld metal in the center os the weld. Columnar grains (of the previous austenite) with primary ferrite in the grain boundaries and acicular ferrite intragranular.
125
ML00119 / Feb.2018
Thermal Fatigue of a Marine Boiler
M - Low Carbon SteelP - Fabrication WeldAp - ShipCd - Thermal Fatigue
Cm - Nital Etched Micrography by OMDf - Ferritic Weld Metal
Micrographic detail of the weld metal in the center os the weld. Columnar grains (of the previous austenite) with primary ferrite in the grain boundaries; and details of the ferrite with aligned second phases and acicular ferrite, intragranular.
112
ML00119 / Feb.2018
Thermal Fatigue of a Marine Boiler
M - Low Carbon SteelP - Fabrication WeldAp - ShipCd - Thermal Fatigue
Cm - Nital Etched Micrography by OMDf - Ferritic Weld Metal

+12 more from this case →

ML00104 — Thermal Fatigue of a Boiler TubeM - Low Carbon SteelP - Autogenously Welded TubeAp - BoilerCd - Thermal Fatigue
The micrography of the longitudinal section of the tube, close to ID, shows the paralel cracks, filled with oxides, perpendicular to the surface.
229
ML00104 / Dec.2017
Thermal Fatigue of a Boiler Tube
M - Low Carbon SteelP - Autogenously Welded TubeAp - BoilerCd - Thermal Fatigue
Cm - As polished micrographyDf - Close to the Internal Surface
Micrographic details of the longitudinal section of the tube, close to OD, showing paralel cracks, filled with oxides, perpendicular to the surface.
115
ML00104 / Dec.2017
Thermal Fatigue of a Boiler Tube
M - Low Carbon SteelP - Autogenously Welded TubeAp - BoilerCd - Thermal Fatigue
Cm - As polished micrographyDf - Cracks Transverse to the Surface
Micrographic details of the longitudinal section of the tube, close to OD, showing paralel cracks, filled with oxides, perpendicular to the surface.
109
ML00104 / Dec.2017
Thermal Fatigue of a Boiler Tube
M - Low Carbon SteelP - Autogenously Welded TubeAp - BoilerCd - Thermal Fatigue
Cm - As polished micrographyDf - Thermal Fatigue Cracks
Micrographic details of the longitudinal section of the tube, close to ID, showing paralel cracks, filled with oxides, perpendicular to the surface.
103
ML00104 / Dec.2017
Thermal Fatigue of a Boiler Tube
M - Low Carbon SteelP - Autogenously Welded TubeAp - BoilerCd - Thermal Fatigue
Cm - As polished micrographyDf - Cracks Transverse to the Surface
ML00104 / Dec.2017
Thermal Fatigue of a Boiler Tube
M - Low Carbon SteelP - Autogenously Welded TubeAp - BoilerCd - Thermal Fatigue
Cm - As polished micrographyDf - Thermal Fatigue Cracks

+10 more from this case →