Nital Etched Micrography by OM
1 case · 4 images
Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00110 / Jan.2018
Non Conformance in Spray and Fuse Pin
M - Low Alloy Medium Carbon QTP - Tubular ForgingAp - O&G Well DrillingCd - Heat Treatment Defect
Cm - Nital Etched Micrography by OMDf - Ferrite and Pearlite
More from these cases

ML00110 / Jan.2018
Non Conformance in Spray and Fuse Pin
M - Low Alloy Medium Carbon QTP - Tubular ForgingAp - O&G Well DrillingCd - Heat Treatment Defect
Cm - Nital Etched Micrography by OMDf - Base Metal

ML00110 / Jan.2018
Non Conformance in Spray and Fuse Pin
M - Low Alloy Medium Carbon QTP - Tubular ForgingAp - O&G Well DrillingCd - Heat Treatment Defect
Cm - Nital Etched Micrography by OMDf - Ferrite and Pearlite

ML00110 / Jan.2018
Non Conformance in Spray and Fuse Pin
M - Low Alloy Medium Carbon QTP - Tubular ForgingAp - O&G Well DrillingCd - Heat Treatment Defect
Cm - Nital Etched Micrography by OMDf - Ferrite and Pearlite