Nital Etched Micrography by OM
4 cases · 5 images
Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00172 / Mar.2021
Brittle Fracture of a LAS Valve Spring
M - Low Alloy Medium Carbon QTP - SpringAp - Oil and GasCd - Brittle Fracture
Cm - Nital Etched Micrography by OMDf - Transverse Section

ML00103 / Nov.2017
Brittle Fracture of a Free-Cutting Connector
M - Low Carbon SteelP - Machined PartAp - ShipCd - Brittle Fracture
Cm - Nital Etched Micrography by OMDf - Transverse Section

ML00096 / Oct.2017
Carbon Steel Tee Rail
M - High Strength Low AlloyP - RailAp - TransportationCd - Typical manufacturing
Cm - Nital Etched Micrography by OMDf - Transverse Section

ML00091 / Sep.2017
Flat Bottom Rail TR57
M - High Strength Low AlloyP - RailAp - TransportationCd - Typical manufacturing
Cm - Nital Etched Micrography by OMDf - Transverse Section
More from these cases

ML00172 / Mar.2021
Brittle Fracture of a LAS Valve Spring
M - Low Alloy Medium Carbon QTP - SpringAp - Oil and GasCd - Brittle Fracture
Cm - Nital Etched Micrography by OMDf - Transverse Section