Kalling Etched Micrography by OM

3 cases · 9 images for “corrosion”

Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00121 / Feb.2018
Pitting Corrosion in a Subsea System
M - Austenitic / MartensiticP - Rod & CylinderAp - SubseaCd - Pitting Corrosion
Cm - Kalling Etched Micrography by OMDf - Martensite
ML00085 / Nov.2017
Corrosion Fatigue of a Martensitic SS Pin
M - Martensitic Stainless SteelP - Forged PinAp - O&G Well DrillingCd - Corrosion Fatigue
Cm - Kalling Etched Micrography by OMDf - Martensite
Microstructure of the fitting in the transverse section, presenting a granular Ni austenitic structure.  No evidences of any phase in the grain boundaries.
114
ML00011 / Oct.2017
Intergranular SCC of Pure Nickel
M - Unalloyed NickelP - Wrought FittingAp - Chemical IndustryCd - Stress Corrosion
Cm - Kalling Etched Micrography by OMDf - Austenite

More from these cases

ML00121 — Pitting Corrosion in a Subsea SystemM - Austenitic / MartensiticP - Rod & CylinderAp - SubseaCd - Pitting Corrosion
ML00121 / Feb.2018
Pitting Corrosion in a Subsea System
M - Austenitic / MartensiticP - Rod & CylinderAp - SubseaCd - Pitting Corrosion
Cm - Kalling Etched Micrography by OMDf - Martensite
ML00121 / Feb.2018
Pitting Corrosion in a Subsea System
M - Austenitic / MartensiticP - Rod & CylinderAp - SubseaCd - Pitting Corrosion
Cm - Kalling Etched Micrography by OMDf - Martensite
ML00085 — Corrosion Fatigue of a Martensitic SS PinM - Martensitic Stainless SteelP - Forged PinAp - O&G Well DrillingCd - Corrosion Fatigue
ML00085 / Nov.2017
Corrosion Fatigue of a Martensitic SS Pin
M - Martensitic Stainless SteelP - Forged PinAp - O&G Well DrillingCd - Corrosion Fatigue
Cm - Kalling Etched Micrography by OMDf - Banded Structure
ML00085 / Nov.2017
Corrosion Fatigue of a Martensitic SS Pin
M - Martensitic Stainless SteelP - Forged PinAp - O&G Well DrillingCd - Corrosion Fatigue
Cm - Kalling Etched Micrography by OMDf - Martensite
ML00011 — Intergranular SCC of Pure NickelM - Unalloyed NickelP - Wrought FittingAp - Chemical IndustryCd - Stress Corrosion
Microstructure of the fitting in the transverse section, presenting a granular Ni austenitic structure.  No evidences of any phase in the grain boundaries.
110
ML00011 / Oct.2017
Intergranular SCC of Pure Nickel
M - Unalloyed NickelP - Wrought FittingAp - Chemical IndustryCd - Stress Corrosion
Cm - Kalling Etched Micrography by OMDf - Austenite
ML00011 / Oct.2017
Intergranular SCC of Pure Nickel
M - Unalloyed NickelP - Wrought FittingAp - Chemical IndustryCd - Stress Corrosion
Cm - Kalling Etched Micrography by OMDf - Austenite