Crevice Corrosion in a Subsea System — Aspect Before Analysis

The macrography of the longitudinal section of the pin (9.5 mm nominal diameter) shows the localized corrosion associated to the non metallic inclusions.
107
ML00016 / Apr.2017
SCC in Free Cutting 303SS
M - Austenitic Stainless SteelP - Machined PartAp - OffshoreCd - Stress Corrosion
Cm - Macro Oxalic Acid Electrolytic EtchedDf - Localized Corrosion