Structure

1 case · 1 image

Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00010 / Oct.2017
Cold Cracks in a Gouged Weld Metal
M - Low Alloy Low Carbon QTP - Rolled PlateAp - OffshoreCd - Welding Defect
Cm - Nital Etched Micrography by OMDf - Transverse Section