Ship

1 case · 1 image

Crevice Corrosion in a Subsea System — Aspect Before Analysis

Aspect of the 4" pipe that was in seawater service for 8 years and leaked in a longitudinal line that corresponds to the seam weld. The internal surface presented thick deposits. Although the pipe was cut with a thermal process, the analysis was conducted after mechanical cutting.
100
ML00140 / May.2019
Preferential Corrosion of Pipe Seam Weld
M - Low Carbon SteelP - Longitudinal Seam Welded PipeAp - ShipCd - Preferential Dissolution
Cm - Aspect Before AnalysisDf - General View