Ship
1 case · 3 images
Crevice Corrosion in a Subsea System — Aspect Before Analysis
Condition: Brittle Behavior ×Microstructure: Ferritic matrix ×Capture method: Optical Microscope ×clear all

ML00040 / Apr.2017
Brittle Fracture of a Valve Stem
M - Nodular Cast IronP - Valve StemAp - ShipCd - Brittle Fracture
Cm - Nital Etched Micrography by OMDf - Graphite in Nodules
More from these cases

ML00040 / Apr.2017
Brittle Fracture of a Valve Stem
M - Nodular Cast IronP - Valve StemAp - ShipCd - Brittle Fracture
Cm - Nital Etched Micrography by OMDf - Fracture

ML00040 / Apr.2017
Brittle Fracture of a Valve Stem
M - Nodular Cast IronP - Valve StemAp - ShipCd - Brittle Fracture
Cm - Nital Etched Micrography by OMDf - Fracture