Oil and Gas

2 cases · 4 images

Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00175 / Aug.2021
Localized External Wear of a Wire Rope
M - High Carbon SteelP - Wire RopeAp - Oil and GasCd - Wear
Cm - Transverse Section AspectDf - Plastic Deformation
ML00152 / Dec.2018
Low Alloy Steel Pump Shaft
M - High Strength Low AlloyP - ShaftAp - Oil and GasCd - Removed From Service
Cm - NItal Etched MacroDf - Longitudinal Section

More from these cases

ML00175 — Localized External Wear of a Wire RopeM - High Carbon SteelP - Wire RopeAp - Oil and GasCd - Wear
ML00175 / Aug.2021
Localized External Wear of a Wire Rope
M - High Carbon SteelP - Wire RopeAp - Oil and GasCd - Wear
Cm - Transverse Section AspectDf - General View
ML00175 / Aug.2021
Localized External Wear of a Wire Rope
M - High Carbon SteelP - Wire RopeAp - Oil and GasCd - Wear
Cm - Transverse Section AspectDf - General View