Crevice Corrosion in a Subsea System — Aspect Before Analysis

Fracture appearance in a sheared region, presenting a ductile morphology for the fracture micromechanism.
109
ML00046 / Jan.2018
Brittle Fracture of SS Shear Pin
M - Martensitic Stainless SteelP - Machined PartAp - EnergyCd - Intergranular Cracking
Cm - Fractography by SEMDf - Ductile Fracture