Crevice Corrosion in a Subsea System — Aspect Before Analysis
Condition: Casting Defect ×Capture method: Optical Microscope ×Detail focus: Microstructure ×clear all

ML00017 / Apr.2017
Casting Defect in CA6NM
M - Martensitic Stainless SteelP - Machined PartAp - EnergyCd - Casting Defect
Cm - Micrography by OMDf - Non Metallic Inclusions
More from these cases

ML00017 / Apr.2017
Casting Defect in CA6NM
M - Martensitic Stainless SteelP - Machined PartAp - EnergyCd - Casting Defect
Cm - Kalling Etched Micrography by OMDf - Delta Ferrite Islands

ML00017 / Apr.2017
Casting Defect in CA6NM
M - Martensitic Stainless SteelP - Machined PartAp - EnergyCd - Casting Defect
Cm - Kalling Etched Micrography by OMDf - Coarse Structure

ML00017 / Apr.2017
Casting Defect in CA6NM
M - Martensitic Stainless SteelP - Machined PartAp - EnergyCd - Casting Defect
Cm - Kalling Etched Micrography by OMDf - Delta Ferrite Islands

ML00017 / Apr.2017
Casting Defect in CA6NM
M - Martensitic Stainless SteelP - Machined PartAp - EnergyCd - Casting Defect
Cm - Kalling Etched Micrography by OMDf - Non Metallic Inclusions