“brittle fracture”

3 cases · 8 images for “brittle fracture”

Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00172 / Mar.2021
Brittle Fracture of a LAS Valve Spring
M - Low Alloy Medium Carbon QTP - SpringAp - Oil and GasCd - Brittle Fracture
Cm - Aspect Before AnalysisDf - Corrosion
ML00141 / Jul.2018
Brittle Fracture of a Corroded Gray Cast Iron
M - Gray Cast ironP - CastingAp - EngineCd - Brittle Fracture
Cm - Fractography by SEMDf - Corrosion
ML00137 / Mar.2021
Brittle Fracture of a 15-5 PH Valve Spring
M - Precipitation Hardened Stainless SteelP - SpringAp - Oil and GasCd - Brittle Behavior
Cm - Surface Aspect by SEMDf - Corrosion

More from these cases

ML00172 — Brittle Fracture of a LAS Valve SpringM - Low Alloy Medium Carbon QTP - SpringAp - Oil and GasCd - Brittle Fracture
ML00172 / Mar.2021
Brittle Fracture of a LAS Valve Spring
M - Low Alloy Medium Carbon QTP - SpringAp - Oil and GasCd - Brittle Fracture
Cm - Surface Aspect by SEMDf - Corrosion
ML00141 — Brittle Fracture of a Corroded Gray Cast IronM - Gray Cast ironP - CastingAp - EngineCd - Brittle Fracture
ML00141 / Jul.2018
Brittle Fracture of a Corroded Gray Cast Iron
M - Gray Cast ironP - CastingAp - EngineCd - Brittle Fracture
Cm - As polished micrographyDf - Corrosion
ML00141 / Jul.2018
Brittle Fracture of a Corroded Gray Cast Iron
M - Gray Cast ironP - CastingAp - EngineCd - Brittle Fracture
Cm - As polished micrographyDf - Corrosion
ML00141 / Jul.2018
Brittle Fracture of a Corroded Gray Cast Iron
M - Gray Cast ironP - CastingAp - EngineCd - Brittle Fracture
Cm - Nital Etched Micrography by OMDf - Corrosion
ML00137 — Brittle Fracture of a 15-5 PH Valve SpringM - Precipitation Hardened Stainless SteelP - SpringAp - Oil and GasCd - Brittle Behavior
ML00137 / Mar.2021
Brittle Fracture of a 15-5 PH Valve Spring
M - Precipitation Hardened Stainless SteelP - SpringAp - Oil and GasCd - Brittle Behavior
Cm - Surface Aspect by SEMDf - Corrosion