“stress corrosion”

5 cases · 58 images for “stress corrosion”

Crevice Corrosion in a Subsea System — Aspect Before Analysis

Aspect of the stub end, that is used in combination with a lap joint flange.  In this case it was prepared from a seam welded pipe, longitudinal, also with circunferential weld to the stub face (which means it was not flared).  The cracking is circunferential in the non painted region, not associated to any welded area.
435
ML00168 / Aug.2020
SCC of Austenitic SS Flange Stub End
M - Austenitic Stainless SteelP - Stub EndAp - Chemical IndustryCd - Stress Corrosion
Cm - Aspect Before AnalysisDf - General View
Optical micrography of a longitudinal section of the fractured bolt, at the thread.  The material is austenitic, free from carbides, and the threads were almost removed by the stress corrosion cracks.
757
ML00157 / Feb.2020
Bolts Under Chloride SCC Conditions
M - Austenitic Stainless SteelP - BoltAp - Oil and GasCd - Stress Corrosion
Cm - Oxalic Acid Electrolytic EtchDf - Stress Corrosion Cracks
Aspect of the heat exchanger plate showing the rupture of the plate in multiple cracks, starting at the side of the crude oil with high salinity.
729
ML00051 / Apr.2020
Chloride SCC of 316 Heat Exchanger Plate
M - Austenitic Stainless SteelP - Heat Exchanger PartAp - FPSOCd - Stress Corrosion
Cm - Aspect Before AnalysisDf - Cracking
Regions of the pin thread presenting pitting corrosion.
635
ML00016 / Apr.2017
SCC in Free Cutting 303SS
M - Austenitic Stainless SteelP - Machined PartAp - OffshoreCd - Stress Corrosion
Cm - Surface Aspect by SEMDf - Localized Corrosion
Transverse section of the fitting that suffered a longitudinal cracking. As polished. The wrought fitting has suffered intergranular stress corrosion cracking from the internal surface, exposed to hot caustic environment.
566
ML00011 / Oct.2017
Intergranular SCC of Pure Nickel
M - Unalloyed NickelP - Wrought FittingAp - Chemical IndustryCd - Stress Corrosion
Cm - Micrography by OMDf - Intergranular Cracking

More from these cases

ML00168 — SCC of Austenitic SS Flange Stub EndM - Austenitic Stainless SteelP - Stub EndAp - Chemical IndustryCd - Stress Corrosion
ML00168 / Aug.2020
SCC of Austenitic SS Flange Stub End
M - Austenitic Stainless SteelP - Stub EndAp - Chemical IndustryCd - Stress Corrosion
Cm - Aspect Before AnalysisDf - Cracking
ML00168 / Aug.2020
SCC of Austenitic SS Flange Stub End
M - Austenitic Stainless SteelP - Stub EndAp - Chemical IndustryCd - Stress Corrosion
Cm - Oxalic Acid Electrolytic EtchDf - Longitudinal Section
ML00168 / Aug.2020
SCC of Austenitic SS Flange Stub End
M - Austenitic Stainless SteelP - Stub EndAp - Chemical IndustryCd - Stress Corrosion
Cm - Oxalic Acid Electrolytic EtchDf - Austenite
ML00168 / Aug.2020
SCC of Austenitic SS Flange Stub End
M - Austenitic Stainless SteelP - Stub EndAp - Chemical IndustryCd - Stress Corrosion
Cm - Oxalic Acid Electrolytic EtchDf - Austenite
ML00168 / Aug.2020
SCC of Austenitic SS Flange Stub End
M - Austenitic Stainless SteelP - Stub EndAp - Chemical IndustryCd - Stress Corrosion
Cm - Longitudinal Section AspectDf - Multiple cracks

+10 more from this case →

ML00157 — Bolts Under Chloride SCC ConditionsM - Austenitic Stainless SteelP - BoltAp - Oil and GasCd - Stress Corrosion
Aspect of a 5/16" bolt manufactured in an AISI 316 austenitic stainless steel, that was also operating inside the pressure vessel, but was not yet damaged.  It is a hexagonal head bolt, 1 1/2" long, fastened with a hexagonal nut and a lock washer.
118
ML00157 / Feb.2020
Bolts Under Chloride SCC Conditions
M - Austenitic Stainless SteelP - BoltAp - Oil and GasCd - Stress Corrosion
Cm - Aspect Before AnalysisDf - General View
Low magnification micrography, by optical microscope, of the longitudinal section of a damaged bolt, in the center of the thickness. The microstructure is austenitic, free from carbides.
100
ML00157 / Feb.2020
Bolts Under Chloride SCC Conditions
M - Austenitic Stainless SteelP - BoltAp - Oil and GasCd - Stress Corrosion
Cm - Oxalic Acid Electrolytic EtchDf - Austenite
ML00157 / Feb.2020
Bolts Under Chloride SCC Conditions
M - Austenitic Stainless SteelP - BoltAp - Oil and GasCd - Stress Corrosion
Cm - Nital Etched Micrography by OMDf - Strain Hardened
ML00157 / Feb.2020
Bolts Under Chloride SCC Conditions
M - Austenitic Stainless SteelP - BoltAp - Oil and GasCd - Stress Corrosion
Cm - Oxalic Acid Electrolytic EtchDf - Strain Hardened
ML00157 / Feb.2020
Bolts Under Chloride SCC Conditions
M - Austenitic Stainless SteelP - BoltAp - Oil and GasCd - Stress Corrosion
Cm - Aspect Before AnalysisDf - Fracture

+8 more from this case →

ML00051 — Chloride SCC of 316 Heat Exchanger PlateM - Austenitic Stainless SteelP - Heat Exchanger PartAp - FPSOCd - Stress Corrosion
Macrography of the surface of the cracked heat exchanger plate, manufactured in austenitic stainless steel.
159
ML00051 / Apr.2020
Chloride SCC of 316 Heat Exchanger Plate
M - Austenitic Stainless SteelP - Heat Exchanger PartAp - FPSOCd - Stress Corrosion
Cm - Macro Oxalic Acid Electrolytic EtchedDf - Cracking
Micrography of the plate material presenting a granular austenitic structure, free from precipitation.
122
ML00051 / Apr.2020
Chloride SCC of 316 Heat Exchanger Plate
M - Austenitic Stainless SteelP - Heat Exchanger PartAp - FPSOCd - Stress Corrosion
Cm - Eletrolytically Etched Micrography by OMDf - Austenite
Micrographic detail of the austenitic microstructure of the heat exchanger plate, free from carbides that suggest the adoption of a material in a solution annealed condition, although the high hardness level indicates cold working.
109
ML00051 / Apr.2020
Chloride SCC of 316 Heat Exchanger Plate
M - Austenitic Stainless SteelP - Heat Exchanger PartAp - FPSOCd - Stress Corrosion
Cm - Eletrolytically Etched Micrography by OMDf - Austenite
Micrography presenting the transgranular morphology of the stress corrosion cracks of the austenitic plate.  EDS analysis at the plate surface indicated high Cl peaks.
111
ML00051 / Apr.2020
Chloride SCC of 316 Heat Exchanger Plate
M - Austenitic Stainless SteelP - Heat Exchanger PartAp - FPSOCd - Stress Corrosion
Cm - Eletrolytically Etched Micrography by OMDf - Corrosion Cracking
ML00051 / Apr.2020
Chloride SCC of 316 Heat Exchanger Plate
M - Austenitic Stainless SteelP - Heat Exchanger PartAp - FPSOCd - Stress Corrosion
Cm - Micrography by OM using A262 Method ADf - Corrosion Cracking
ML00016 — SCC in Free Cutting 303SSM - Austenitic Stainless SteelP - Machined PartAp - OffshoreCd - Stress Corrosion
Regions of the localized corrosion spots associated to non metallic inclusions.
123
ML00016 / Apr.2017
SCC in Free Cutting 303SS
M - Austenitic Stainless SteelP - Machined PartAp - OffshoreCd - Stress Corrosion
Cm - Surface Aspect by SEMDf - Non Metallic Inclusions
The macrography of the longitudinal section of the pin (9.5 mm nominal diameter) shows the localized corrosion associated to the non metallic inclusions.
107
ML00016 / Apr.2017
SCC in Free Cutting 303SS
M - Austenitic Stainless SteelP - Machined PartAp - OffshoreCd - Stress Corrosion
Cm - Macro Oxalic Acid Electrolytic EtchedDf - Localized Corrosion
ML00016 / Apr.2017
SCC in Free Cutting 303SS
M - Austenitic Stainless SteelP - Machined PartAp - OffshoreCd - Stress Corrosion
Cm - Micrography by OM using A262 Method ADf - Localized Corrosion
ML00016 / Apr.2017
SCC in Free Cutting 303SS
M - Austenitic Stainless SteelP - Machined PartAp - OffshoreCd - Stress Corrosion
Cm - Micrography by OM using A262 Method ADf - Non Metallic Inclusions
ML00016 / Apr.2017
SCC in Free Cutting 303SS
M - Austenitic Stainless SteelP - Machined PartAp - OffshoreCd - Stress Corrosion
Cm - Micrography by OM using A262 Method ADf - Localized Corrosion

+3 more from this case →

ML00011 — Intergranular SCC of Pure NickelM - Unalloyed NickelP - Wrought FittingAp - Chemical IndustryCd - Stress Corrosion
The fitting presented through wall cracks that lead to leaking.  The internal aspect of the surface is presented where the cracks were still in the begining.
127
ML00011 / Oct.2017
Intergranular SCC of Pure Nickel
M - Unalloyed NickelP - Wrought FittingAp - Chemical IndustryCd - Stress Corrosion
Cm - Aspect Before AnalysisDf - Crack
Microstructure of the fitting in the transverse section, presenting a granular Ni austenitic structure.  No evidences of any phase in the grain boundaries.
114
ML00011 / Oct.2017
Intergranular SCC of Pure Nickel
M - Unalloyed NickelP - Wrought FittingAp - Chemical IndustryCd - Stress Corrosion
Cm - Kalling Etched Micrography by OMDf - Austenite
Microstructure of the fitting in the transverse section, presenting a granular Ni austenitic structure.  No evidences of any phase in the grain boundaries.
110
ML00011 / Oct.2017
Intergranular SCC of Pure Nickel
M - Unalloyed NickelP - Wrought FittingAp - Chemical IndustryCd - Stress Corrosion
Cm - Kalling Etched Micrography by OMDf - Austenite
ML00011 / Oct.2017
Intergranular SCC of Pure Nickel
M - Unalloyed NickelP - Wrought FittingAp - Chemical IndustryCd - Stress Corrosion
Cm - Kalling Etched Micrography by OMDf - Austenite
After opening the crack the fracture surface presented different aspects close to the internal surface and through the wall propagation.  Intergranular at the surface, showing intergranular SCC mechanism, and transgranular with striation, showing the contribution of pulsing loads.
101
ML00011 / Oct.2017
Intergranular SCC of Pure Nickel
M - Unalloyed NickelP - Wrought FittingAp - Chemical IndustryCd - Stress Corrosion
Cm - Fractography by SEMDf - Through Wall Cracking

+7 more from this case →