Atlas

22 cases · 44 images

Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00184 / Apr.2023
Dissimilar Steels in a Threaded Connection
M - Low Carbon SteelP - ForgingAp - OffshoreCd - Localized Dissolution
Cm - Transverse Section AspectDf - Corrosion
ML00181 / Apr.2022
Wear of a Carburized Hypoid Gear
M - Low Alloy for Thermochemical TreatmentP - Pinion-crown assemblyAp - ShipCd - Wear
Cm - Transverse Section AspectDf - Fatigue Crack
ML00180 / Mar.2022
Local Melting of Copper Cooling Tubes
M - Pure CopperP - Cooling TubeAp - SiderurgyCd - Overheating
Cm - Transverse Section AspectDf - Localized Thinning
ML00175 / Aug.2021
Localized External Wear of a Wire Rope
M - High Carbon SteelP - Wire RopeAp - Oil and GasCd - Wear
Cm - Transverse Section AspectDf - Plastic Deformation
ML00170 / Sep.2020
MIC in Aluminum Brass Tubes
M - Aluminum BrassP - Seamless tubeAp - MaritimeCd - Preferential Dissolution
Cm - Transverse Section AspectDf - Localized Thinning
ML00168 / Aug.2020
SCC of Austenitic SS Flange Stub End
M - Austenitic Stainless SteelP - Stub EndAp - Chemical IndustryCd - Stress Corrosion
Cm - Transverse Section AspectDf - Cracks
Throught wall cracking of the waterwall tube at the leakage position, thick edged,  The external surface of the tube was grounded to remove the membrane and the cracking is associated to the tube attachement.
242
ML00163 / Jun.2020
Corrosion Fatigue of a Boiler Waterwall Tube
M - Low Carbon SteelP - Seamless tubeAp - BoilerCd - Corrosion Fatigue
Cm - Transverse Section AspectDf - Thick-edged rupture
ML00160 / Apr.2020
High Temperature Degradation of 310SS
M - Austenitic Stainless SteelP - Rectangular TubeAp - Chemical IndustryCd - Scaling
Cm - Transverse Section AspectDf - Thinning

More from these cases

ML00184 — Dissimilar Steels in a Threaded ConnectionM - Low Carbon SteelP - ForgingAp - OffshoreCd - Localized Dissolution
ML00184 / Apr.2023
Dissimilar Steels in a Threaded Connection
M - Low Carbon SteelP - ForgingAp - OffshoreCd - Localized Dissolution
Cm - Transverse Section AspectDf - Localized Corrosion
ML00180 — Local Melting of Copper Cooling TubesM - Pure CopperP - Cooling TubeAp - SiderurgyCd - Overheating
ML00180 / Mar.2022
Local Melting of Copper Cooling Tubes
M - Pure CopperP - Cooling TubeAp - SiderurgyCd - Overheating
Cm - Transverse Section AspectDf - Leakage
ML00180 / Mar.2022
Local Melting of Copper Cooling Tubes
M - Pure CopperP - Cooling TubeAp - SiderurgyCd - Overheating
Cm - Transverse Section AspectDf - Thinning
ML00180 / Mar.2022
Local Melting of Copper Cooling Tubes
M - Pure CopperP - Cooling TubeAp - SiderurgyCd - Overheating
Cm - Transverse Section AspectDf - Leakage
ML00175 — Localized External Wear of a Wire RopeM - High Carbon SteelP - Wire RopeAp - Oil and GasCd - Wear
ML00175 / Aug.2021
Localized External Wear of a Wire Rope
M - High Carbon SteelP - Wire RopeAp - Oil and GasCd - Wear
Cm - Transverse Section AspectDf - General View
ML00175 / Aug.2021
Localized External Wear of a Wire Rope
M - High Carbon SteelP - Wire RopeAp - Oil and GasCd - Wear
Cm - Transverse Section AspectDf - General View
ML00170 — MIC in Aluminum Brass TubesM - Aluminum BrassP - Seamless tubeAp - MaritimeCd - Preferential Dissolution
ML00170 / Sep.2020
MIC in Aluminum Brass Tubes
M - Aluminum BrassP - Seamless tubeAp - MaritimeCd - Preferential Dissolution
Cm - Transverse Section AspectDf - Localized Thinning