Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00170 / Sep.2020
MIC in Aluminum Brass Tubes
M - Aluminum BrassP - Seamless tubeAp - MaritimeCd - Preferential Dissolution
Cm - Surface AspectDf - Internal Surface
Aspect of the internal tube surface after a longitudinal cut, without cleaning.  It is possible to see a clean surface inside the tube.
104
ML00165 / Jul.2020
SCC of Aluminum Bronze Heating Coil
M - Aluminum BronzeP - Seamless tubeAp - Oil and GasCd - Stress Corrosion
Cm - Surface AspectDf - Internal Surface