“corrosion”

5 cases · 13 images for “corrosion”

Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00165 / Jul.2020
SCC of Aluminum Bronze Heating Coil
M - Aluminum BronzeP - Seamless tubeAp - Oil and GasCd - Stress Corrosion
Cm - Fractography by SEMDf - Stress Corrosion Cracks
ML00157 / Feb.2020
Bolts Under Chloride SCC Conditions
M - Austenitic Stainless SteelP - BoltAp - Oil and GasCd - Stress Corrosion
Cm - Surface Aspect by SEMDf - Brittle Cracks
Micrography of a transverse section of the shell plate in a cracked position showing the transgranular morphology of the stress corrosion cracks.
167
ML00019 / Apr.2017
Transgranular SCC in Boiler Steam Drum
M - CMn SteelP - Rolled PlateAp - BoilerCd - Stress Corrosion
Cm - Nital Etched Micrography by SEMDf - Transgranular Cracking
Regions of the pin thread presenting pitting corrosion.
635
ML00016 / Apr.2017
SCC in Free Cutting 303SS
M - Austenitic Stainless SteelP - Machined PartAp - OffshoreCd - Stress Corrosion
Cm - Surface Aspect by SEMDf - Localized Corrosion
After opening the crack the fracture surface presented different aspects close to the internal surface and through the wall propagation.  Intergranular at the surface, showing intergranular SCC mechanism, and transgranular with striation, showing the contribution of pulsing loads.
101
ML00011 / Oct.2017
Intergranular SCC of Pure Nickel
M - Unalloyed NickelP - Wrought FittingAp - Chemical IndustryCd - Stress Corrosion
Cm - Fractography by SEMDf - Through Wall Cracking

More from these cases

ML00165 — SCC of Aluminum Bronze Heating CoilM - Aluminum BronzeP - Seamless tubeAp - Oil and GasCd - Stress Corrosion
ML00165 / Jul.2020
SCC of Aluminum Bronze Heating Coil
M - Aluminum BronzeP - Seamless tubeAp - Oil and GasCd - Stress Corrosion
Cm - Fractography by SEMDf - Stress Corrosion Cracks
ML00157 — Bolts Under Chloride SCC ConditionsM - Austenitic Stainless SteelP - BoltAp - Oil and GasCd - Stress Corrosion
ML00157 / Feb.2020
Bolts Under Chloride SCC Conditions
M - Austenitic Stainless SteelP - BoltAp - Oil and GasCd - Stress Corrosion
Cm - Surface Aspect by SEMDf - Brittle Fracture
ML00019 — Transgranular SCC in Boiler Steam DrumM - CMn SteelP - Rolled PlateAp - BoilerCd - Stress Corrosion
ML00019 / Apr.2017
Transgranular SCC in Boiler Steam Drum
M - CMn SteelP - Rolled PlateAp - BoilerCd - Stress Corrosion
Cm - Nital Etched Micrography by SEMDf - Transgranular Crack
ML00016 — SCC in Free Cutting 303SSM - Austenitic Stainless SteelP - Machined PartAp - OffshoreCd - Stress Corrosion
Regions of the localized corrosion spots associated to non metallic inclusions.
123
ML00016 / Apr.2017
SCC in Free Cutting 303SS
M - Austenitic Stainless SteelP - Machined PartAp - OffshoreCd - Stress Corrosion
Cm - Surface Aspect by SEMDf - Non Metallic Inclusions
ML00016 / Apr.2017
SCC in Free Cutting 303SS
M - Austenitic Stainless SteelP - Machined PartAp - OffshoreCd - Stress Corrosion
Cm - Surface Aspect by SEMDf - Fracture
ML00011 — Intergranular SCC of Pure NickelM - Unalloyed NickelP - Wrought FittingAp - Chemical IndustryCd - Stress Corrosion
ML00011 / Oct.2017
Intergranular SCC of Pure Nickel
M - Unalloyed NickelP - Wrought FittingAp - Chemical IndustryCd - Stress Corrosion
Cm - Fractography by SEMDf - Intergranular Cracking
ML00011 / Oct.2017
Intergranular SCC of Pure Nickel
M - Unalloyed NickelP - Wrought FittingAp - Chemical IndustryCd - Stress Corrosion
Cm - Fractography by SEMDf - Fatigue Striation
ML00011 / Oct.2017
Intergranular SCC of Pure Nickel
M - Unalloyed NickelP - Wrought FittingAp - Chemical IndustryCd - Stress Corrosion
Cm - Fractography by SEMDf - Fatigue Striation