Atlas

1 case · 1 image

Crevice Corrosion in a Subsea System — Aspect Before Analysis

The forged T presented a ferritic perlitic/bainitic structure at the surface, where the replica was conducted. The base material material hardness is 180 HB.
121
ML00071 / Jan.2019
Reheating Cracking of a CrMo Vessel Weld
M - CrMo SteelP - In Field WeldAp - EnergyCd - Welding Defect
Cm - Nital etched, OMDf - Ferrite and Bainite