Atlas

162 cases · 600 images

Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00088 / Dec.2017
Hydrogen Cracking of an API 5D S135 Drill Pipe
M - Low Alloy Medium Carbon QTP - Drill PipeAp - SubseaCd - Hydrogen Embrittlement
Cm - Nital Etched Micrography by OMDf - Martensite
ML00079 / Jul.2017
Hydrogen Cracking of a Maritime Chain Link
M - High Strength Low AlloyP - Chain LinkAp - OffshoreCd - Hydrogen Embrittlement
Cm - Nital Etched Micrography by OMDf - Martensite
ML00077 / Jun.2018
Hydrogen Cracking of LAS Subsea Bolts
M - Low Alloy Medium Carbon QTP - FastenerAp - SubseaCd - Hydrogen Embrittlement
Cm - Nital Etched Micrography by OMDf - Banded Structure
ML00075 / Jun.2018
Hydrogen Cracking of IN 718 Subsea Fasteners
M - NiCrFe AlloyP - StudAp - SubseaCd - Hydrogen Embrittlement
Cm - Kalling Etched Micrography by OMDf - Austenite
ML00074 / Jun.2018
Hydrogen Cracking of a 17-4 PH Subsea Bolt
M - Precipitation Hardened Stainless SteelP - FastenerAp - SubseaCd - Hydrogen Embrittlement
Cm - Kalling Etched Micrography by OMDf - Martensite
ML00073 / Jun.2018
Hydrogen Cracking of a LAS Subsea Fastener
M - Low Alloy Medium Carbon QTP - FastenerAp - SubseaCd - Hydrogen Embrittlement
Cm - Nital Etched Micrography by OMDf - Martensite
ML00072 / Jan.2018
Liquation Cracks in a High Strength Joint
M - Low Alloy Medium Carbon QTP - Longitudinal Seam Welded PipeAp - O&G Well DrillingCd - Welding Defect
Cm - Nital Etched Micrography by OMDf - Martensite
ML00012 / Aug.2017
Vibration Induced Fatigue in a 316/316L SS
M - Austenitic Stainless SteelP - Seamless PipeAp - OffshoreCd - Vibration Induced Fatigue
Cm - Micrography by OM using A262 Method ADf - Austenite

More from these cases

ML00075 — Hydrogen Cracking of IN 718 Subsea FastenersM - NiCrFe AlloyP - StudAp - SubseaCd - Hydrogen Embrittlement
ML00075 / Jun.2018
Hydrogen Cracking of IN 718 Subsea Fasteners
M - NiCrFe AlloyP - StudAp - SubseaCd - Hydrogen Embrittlement
Cm - Kalling Etched Micrography by OMDf - Austenite
ML00074 — Hydrogen Cracking of a 17-4 PH Subsea BoltM - Precipitation Hardened Stainless SteelP - FastenerAp - SubseaCd - Hydrogen Embrittlement
ML00074 / Jun.2018
Hydrogen Cracking of a 17-4 PH Subsea Bolt
M - Precipitation Hardened Stainless SteelP - FastenerAp - SubseaCd - Hydrogen Embrittlement
Cm - Kalling Etched Micrography by OMDf - Martensite
ML00072 — Liquation Cracks in a High Strength JointM - Low Alloy Medium Carbon QTP - Longitudinal Seam Welded PipeAp - O&G Well DrillingCd - Welding Defect
ML00072 / Jan.2018
Liquation Cracks in a High Strength Joint
M - Low Alloy Medium Carbon QTP - Longitudinal Seam Welded PipeAp - O&G Well DrillingCd - Welding Defect
Cm - Nital Etched Micrography by OMDf - Banded Structure