Atlas
39 cases · 68 images
Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00182 / Jul.2022
Brittle Fracture of a LAS Fixing Rod
M - Low Alloy Medium Carbon QTP - StemAp - Mechanical IndustryCd - Brittle Fracture
Cm - Nital Etched Micrography by OMDf - Longitudinal Section

ML00175 / Aug.2021
Localized External Wear of a Wire Rope
M - High Carbon SteelP - Wire RopeAp - Oil and GasCd - Wear
Cm - Nital Etched Micrography by OMDf - Longitudinal Section

ML00171 / Feb.2021
Corrosion Fatigue of U Bolt Pipe Clamp
M - Low Carbon SteelP - BoltAp - ShipCd - Corrosion Fatigue
Cm - Nital Etched Micrography by OMDf - Longitudinal Section

ML00168 / Aug.2020
SCC of Austenitic SS Flange Stub End
M - Austenitic Stainless SteelP - Stub EndAp - Chemical IndustryCd - Stress Corrosion
Cm - Oxalic Acid Electrolytic EtchDf - Longitudinal Section

ML00167 / Aug.2020
Fatigue of a Flared Tubing Connection
M - Austenitic Stainless SteelP - TubingAp - EngineCd - Mechanical Fatigue
Cm - Oxalic Acid Electrolytic EtchDf - Longitudinal Section

ML00155 / Jan.2020
Failure of a Prestressed Concrete Steel Strand
M - High Carbon SteelP - Wire RopeAp - StructureCd - Corrosion Fatigue
Cm - Nital Etched Micrography by OMDf - Longitudinal Section

ML00152 / Dec.2018
Low Alloy Steel Pump Shaft
M - High Strength Low AlloyP - ShaftAp - Oil and GasCd - Removed From Service
Cm - Nital Etched Micrography by OMDf - Longitudinal Section

ML00151 / Dec.2018
Ferritic Stainless Steel of a Flatware Fork
M - Ferritic Stainless SteelP - Foodstuff ArticleAp - KitchenCd - Typical manufacturing
Cm - Micro by OM, HCl + Ethanol + Picric AcidDf - Longitudinal Section
More from these cases

ML00182 / Jul.2022
Brittle Fracture of a LAS Fixing Rod
M - Low Alloy Medium Carbon QTP - StemAp - Mechanical IndustryCd - Brittle Fracture
Cm - Micro by OM, picric acid+FeCl3+H2O etchDf - Longitudinal Section

ML00175 / Aug.2021
Localized External Wear of a Wire Rope
M - High Carbon SteelP - Wire RopeAp - Oil and GasCd - Wear
Cm - Nital Etched Micrography by OMDf - Longitudinal Section

ML00171 / Feb.2021
Corrosion Fatigue of U Bolt Pipe Clamp
M - Low Carbon SteelP - BoltAp - ShipCd - Corrosion Fatigue
Cm - Nital Etched Micrography by OMDf - Longitudinal Section

ML00152 / Dec.2018
Low Alloy Steel Pump Shaft
M - High Strength Low AlloyP - ShaftAp - Oil and GasCd - Removed From Service
Cm - Nital Etched Micrography by OMDf - Longitudinal Section

ML00151 / Dec.2018
Ferritic Stainless Steel of a Flatware Fork
M - Ferritic Stainless SteelP - Foodstuff ArticleAp - KitchenCd - Typical manufacturing
Cm - Micro by OM, HCl + Ethanol + Picric AcidDf - Longitudinal Section