Atlas
2 cases · 22 images
Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00136 / Jun.2018
Hydrogen Cracks of Subsea Studs
M - Low Alloy Medium Carbon QTP - FastenerAp - SubseaCd - Hydrogen Embrittlement
Cm - Nital Etched Micrography by OMDf - Secondary Cracks

ML00075 / Jun.2018
Hydrogen Cracking of IN 718 Subsea Fasteners
M - NiCrFe AlloyP - StudAp - SubseaCd - Hydrogen Embrittlement
Cm - Kalling Etched Micrography by OMDf - Fracture
More from these cases

ML00136 / Jun.2018
Hydrogen Cracks of Subsea Studs
M - Low Alloy Medium Carbon QTP - FastenerAp - SubseaCd - Hydrogen Embrittlement
Cm - Nital Etched Micrography by OMDf - Secondary Cracks

ML00136 / Jun.2018
Hydrogen Cracks of Subsea Studs
M - Low Alloy Medium Carbon QTP - FastenerAp - SubseaCd - Hydrogen Embrittlement
Cm - Nital Etched Micrography by OMDf - Secondary Cracks

ML00136 / Jun.2018
Hydrogen Cracks of Subsea Studs
M - Low Alloy Medium Carbon QTP - FastenerAp - SubseaCd - Hydrogen Embrittlement
Cm - Nital Etched Micrography by OMDf - Crack

ML00136 / Jun.2018
Hydrogen Cracks of Subsea Studs
M - Low Alloy Medium Carbon QTP - FastenerAp - SubseaCd - Hydrogen Embrittlement
Cm - As polished micrographyDf - Cracking

ML00136 / Jun.2018
Hydrogen Cracks of Subsea Studs
M - Low Alloy Medium Carbon QTP - FastenerAp - SubseaCd - Hydrogen Embrittlement
Cm - As polished micrographyDf - Crack

ML00075 / Jun.2018
Hydrogen Cracking of IN 718 Subsea Fasteners
M - NiCrFe AlloyP - StudAp - SubseaCd - Hydrogen Embrittlement
Cm - Kalling Etched Micrography by OMDf - Intergranular Cracking

ML00075 / Jun.2018
Hydrogen Cracking of IN 718 Subsea Fasteners
M - NiCrFe AlloyP - StudAp - SubseaCd - Hydrogen Embrittlement
Cm - Kalling Etched Micrography by OMDf - Secondary Cracks

ML00075 / Jun.2018
Hydrogen Cracking of IN 718 Subsea Fasteners
M - NiCrFe AlloyP - StudAp - SubseaCd - Hydrogen Embrittlement
Cm - Kalling Etched Micrography by OMDf - Brittle Cracks