Crevice Corrosion in a Subsea System — Aspect Before Analysis
Microstructure: Tempered Martensite ×Capture method: Optical Microscope ×Detail focus: Brittle Cracks ×clear all

ML00161 / Mar.2020
Brittle Fracture of a High Strength Socket
M - Medium Carbon Tool SteelP - ToolAp - Oil and GasCd - Brittle Fracture
Cm - Nital Etched Micrography by OMDf - Brittle Cracks

ML00077 / Jun.2018
Hydrogen Cracking of LAS Subsea Bolts
M - Low Alloy Medium Carbon QTP - FastenerAp - SubseaCd - Hydrogen Embrittlement
Cm - Micrography by OMDf - Brittle Cracks
More from these cases

ML00161 / Mar.2020
Brittle Fracture of a High Strength Socket
M - Medium Carbon Tool SteelP - ToolAp - Oil and GasCd - Brittle Fracture
Cm - Nital Etched Micrography by OMDf - Brittle Cracks