Crevice Corrosion in a Subsea System — Aspect Before Analysis

Micrography of the case, observed in the center of the thickness, showing an equiaxial granular austenitic microstructure, free from carbides.  The structure is typical of a 316 SS, in a solution annealed condition.
176
ML00122 / Feb.2018
Crevice Corrosion in a Subsea System
M - Austenitic Stainless SteelP - CaseAp - Oil and GasCd - Crevice
Cm - Micrography by OM using A262 Method ADf - Austenite

More from these cases

ML00122 — Crevice Corrosion in a Subsea SystemM - Austenitic Stainless SteelP - CaseAp - Oil and GasCd - Crevice
Micrographic detail of the fully austenitic granular structure of the case, in the center of the thickness.
158
ML00122 / Feb.2018
Crevice Corrosion in a Subsea System
M - Austenitic Stainless SteelP - CaseAp - Oil and GasCd - Crevice
Cm - Micrography by OM using A262 Method ADf - Austenite