Atlas
3 cases · 7 images
Crevice Corrosion in a Subsea System — Aspect Before Analysis
Product: Fabrication Weld ×Microstructure: Duplex Ferritic Austenitic ×Capture method: Fractography by SEM ×clear all

ML00134 / Aug.2020
Brittle Fracture of a Superduplex Valve Body
M - Super Duplex Stainless SteelP - Fabrication WeldAp - SubseaCd - Brittle Fracture
Cm - Fractography by SEMDf - Cleavage Facets

ML00094 / Sep.2017
MIC of a Subsea Hydraulic Line
M - Super Duplex Stainless SteelP - Fabrication WeldAp - SubseaCd - Brittle Behavior
Cm - Fractography by SEMDf - Transgranular Fracture

ML00002 / Jan.2018
Preferential Dissolution and Cracks in SDSS
M - Super Duplex Stainless SteelP - Fabrication WeldAp - PipingCd - Preferential Dissolution
Cm - Fractography by SEMDf - Cleavage Facets
More from these cases

ML00134 / Aug.2020
Brittle Fracture of a Superduplex Valve Body
M - Super Duplex Stainless SteelP - Fabrication WeldAp - SubseaCd - Brittle Fracture
Cm - Fractography by SEMDf - Cleavage Facets

ML00134 / Aug.2020
Brittle Fracture of a Superduplex Valve Body
M - Super Duplex Stainless SteelP - Fabrication WeldAp - SubseaCd - Brittle Fracture
Cm - Fractography by SEMDf - Secondary Cracks

ML00002 / Jan.2018
Preferential Dissolution and Cracks in SDSS
M - Super Duplex Stainless SteelP - Fabrication WeldAp - PipingCd - Preferential Dissolution
Cm - Fractography by SEMDf - Cleavage Facets

ML00002 / Jan.2018
Preferential Dissolution and Cracks in SDSS
M - Super Duplex Stainless SteelP - Fabrication WeldAp - PipingCd - Preferential Dissolution
Cm - Fractography by SEMDf - Cleavage Facets