ML00074 / Jun.2018
Hydrogen Cracking of a 17-4 PH Subsea Bolt
M - Precipitation Hardened Stainless SteelP - FastenerAp - SubseaCd - Hydrogen Embrittlement
Cm - Fractography by SEMDf - Intergranular Cracking