Atlas

1 case · 1 image

Crevice Corrosion in a Subsea System — Aspect Before Analysis

Detail of the fatigue cracking, staring from the margin of the weld. The crack propagated though wall of the pipe (5 mm).  The larger thickness of the weldolet requires a large amount of deposited weld metal, about 20 mm that is 4 times the pipe thickness. It is an interesting aspect to be considered by designers.
176
ML00150 / Dec.2018
Vibration Induced Fatigue in a SS Oil Piping
M - Duplex Stainless SteelP - PipingAp - FPSOCd - Vibration Induced Fatigue
Cm - Electrolytically Etched MacroDf - Fatigue Crack