Crevice Corrosion in a Subsea System — Aspect Before Analysis

Detail of the flat fracture from the notch at the bottom of the recess. No plastic deformation.
113
ML00182 / Jul.2022
Brittle Fracture of a LAS Fixing Rod
M - Low Alloy Medium Carbon QTP - StemAp - Mechanical IndustryCd - Brittle Fracture
Cm - Aspect Before AnalysisDf - Brittle Fracture
ML00172 / Mar.2021
Brittle Fracture of a LAS Valve Spring
M - Low Alloy Medium Carbon QTP - SpringAp - Oil and GasCd - Brittle Fracture
Cm - Aspect Before AnalysisDf - Brittle Fracture
Aspect of the broken disc spring, 1/4" thick, OD 10". The fracture is flat and transverse to the disc.
604
ML00080 / Sep.2017
MIC of Stacking Disc Springs
M - Low Alloy Medium Carbon QTP - SpringAp - SubseaCd - Brittle Behavior
Cm - Aspect Before AnalysisDf - Brittle Fracture
Aspect of the broken pin after removal from the box end.
125
ML00009 / Sep.2017
Hydrogen Cracking of a 5" Drill Pipe S135
M - Low Alloy Medium Carbon QTP - Drill PipeAp - SubseaCd - Hydrogen Embrittlement
Cm - Aspect Before AnalysisDf - Brittle Fracture

More from these cases

ML00182 — Brittle Fracture of a LAS Fixing RodM - Low Alloy Medium Carbon QTP - StemAp - Mechanical IndustryCd - Brittle Fracture
ML00182 / Jul.2022
Brittle Fracture of a LAS Fixing Rod
M - Low Alloy Medium Carbon QTP - StemAp - Mechanical IndustryCd - Brittle Fracture
Cm - Aspect Before AnalysisDf - Brittle Fracture
ML00009 — Hydrogen Cracking of a 5" Drill Pipe S135M - Low Alloy Medium Carbon QTP - Drill PipeAp - SubseaCd - Hydrogen Embrittlement
ML00009 / Sep.2017
Hydrogen Cracking of a 5" Drill Pipe S135
M - Low Alloy Medium Carbon QTP - Drill PipeAp - SubseaCd - Hydrogen Embrittlement
Cm - Aspect Before AnalysisDf - Brittle Fracture