Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00168 / Aug.2020
SCC of Austenitic SS Flange Stub End
M - Austenitic Stainless SteelP - Stub EndAp - Chemical IndustryCd - Stress Corrosion
Cm - As polished micrographyDf - Close to the External Surface
ML00165 / Jul.2020
SCC of Aluminum Bronze Heating Coil
M - Aluminum BronzeP - Seamless tubeAp - Oil and GasCd - Stress Corrosion
Cm - As polished micrographyDf - Cracking

More from these cases

ML00168 — SCC of Austenitic SS Flange Stub EndM - Austenitic Stainless SteelP - Stub EndAp - Chemical IndustryCd - Stress Corrosion
ML00168 / Aug.2020
SCC of Austenitic SS Flange Stub End
M - Austenitic Stainless SteelP - Stub EndAp - Chemical IndustryCd - Stress Corrosion
Cm - As polished micrographyDf - Multiple cracks
ML00165 — SCC of Aluminum Bronze Heating CoilM - Aluminum BronzeP - Seamless tubeAp - Oil and GasCd - Stress Corrosion
ML00165 / Jul.2020
SCC of Aluminum Bronze Heating Coil
M - Aluminum BronzeP - Seamless tubeAp - Oil and GasCd - Stress Corrosion
Cm - As polished micrographyDf - Intergranular Corrosion
ML00165 / Jul.2020
SCC of Aluminum Bronze Heating Coil
M - Aluminum BronzeP - Seamless tubeAp - Oil and GasCd - Stress Corrosion
Cm - As polished micrographyDf - Through Wall Cracking