Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00143 / Aug.2018
Impact of a .308 Winchester on A36 Plate
M - Low Carbon SteelP - Rolled PlateAp - StructureCd - Pierced
Cm - Longitudinal Section AspectDf - Longitudinal Section
ML00090 / Sep.2017
Carbon Steel Tubing for Structural Application
M - Low Carbon SteelP - TubeAp - StructureCd - Typical manufacturing
Cm - Nital Etched Micrography by OMDf - Longitudinal Section