Atlas

1 case · 1 image

Crevice Corrosion in a Subsea System — Aspect Before Analysis

The main pipe, ND 18", has suffered a pipe through wall cracking at the margin of the 1 1/2" branch socket weld.
664
ML00006 / Apr.2017
Vibration Induced Fatigue in 304SS
M - Austenitic Stainless SteelP - Longitudinal Seam Welded PipeAp - PipingCd - Vibration Induced Fatigue
Cm - Aspect Before AnalysisDf - Crack