Atlas

2 cases · 4 images

Crevice Corrosion in a Subsea System — Aspect Before Analysis

Longitudinal section of the main pipe showing as austenitic structure with small amount of delta ferrite, aligned. The white band in the center of the figure is a segregation band that was not fully etched.
133
ML00006 / Apr.2017
Vibration Induced Fatigue in 304SS
M - Austenitic Stainless SteelP - Longitudinal Seam Welded PipeAp - PipingCd - Vibration Induced Fatigue
Cm - Micrography by OM using A262 Method ADf - Austenite
Austenitic structure at the transverse section of the pipe, free from carbides.
277
ML00014 / Apr.2017
Pitting Corrosion in 316SS Pipe
M - Austenitic Stainless SteelP - Seamless PipeAp - FPSOCd - Pitting Corrosion
Cm - Micrography by OM using A262 Method ADf - Austenite

More from these cases

ML00006 — Vibration Induced Fatigue in 304SSM - Austenitic Stainless SteelP - Longitudinal Seam Welded PipeAp - PipingCd - Vibration Induced Fatigue
Longitudinal section of the main pipe showing as austenitic structure with small amount of delta ferrite, aligned (black dots).
117
ML00006 / Apr.2017
Vibration Induced Fatigue in 304SS
M - Austenitic Stainless SteelP - Longitudinal Seam Welded PipeAp - PipingCd - Vibration Induced Fatigue
Cm - Micrography by OM using A262 Method ADf - Austenite
ML00014 — Pitting Corrosion in 316SS PipeM - Austenitic Stainless SteelP - Seamless PipeAp - FPSOCd - Pitting Corrosion
Austenitic structure, free from carbides, exactly in the region of the pitting, indicating that the corrosion is not associated to the material microstructure.
261
ML00014 / Apr.2017
Pitting Corrosion in 316SS Pipe
M - Austenitic Stainless SteelP - Seamless PipeAp - FPSOCd - Pitting Corrosion
Cm - Micrography by OM using A262 Method ADf - Austenite