Crevice Corrosion in a Subsea System — Aspect Before Analysis
Application: Energy ×Microstructure: Tempered Martensite ×Capture method: Kalling Etched Micrography by OM ×clear all

ML00124 / Feb.2018
MIC of a Martensitic Valve Ring
M - Martensitic Stainless SteelP - ForgingAp - EnergyCd - Brittle Behavior
Cm - Kalling Etched Micrography by OMDf - Martensite

ML00046 / Jan.2018
Brittle Fracture of SS Shear Pin
M - Martensitic Stainless SteelP - Machined PartAp - EnergyCd - Intergranular Cracking
Cm - Kalling Etched Micrography by OMDf - Martensite, delta ferrite & carbides
More from these cases

ML00124 / Feb.2018
MIC of a Martensitic Valve Ring
M - Martensitic Stainless SteelP - ForgingAp - EnergyCd - Brittle Behavior
Cm - Kalling Etched Micrography by OMDf - Martensite

ML00124 / Feb.2018
MIC of a Martensitic Valve Ring
M - Martensitic Stainless SteelP - ForgingAp - EnergyCd - Brittle Behavior
Cm - Kalling Etched Micrography by OMDf - Crack

ML00124 / Feb.2018
MIC of a Martensitic Valve Ring
M - Martensitic Stainless SteelP - ForgingAp - EnergyCd - Brittle Behavior
Cm - Kalling Etched Micrography by OMDf - Intergranular Cracking

ML00124 / Feb.2018
MIC of a Martensitic Valve Ring
M - Martensitic Stainless SteelP - ForgingAp - EnergyCd - Brittle Behavior
Cm - Kalling Etched Micrography by OMDf - Crack

ML00124 / Feb.2018
MIC of a Martensitic Valve Ring
M - Martensitic Stainless SteelP - ForgingAp - EnergyCd - Brittle Behavior
Cm - Kalling Etched Micrography by OMDf - Crack

ML00046 / Jan.2018
Brittle Fracture of SS Shear Pin
M - Martensitic Stainless SteelP - Machined PartAp - EnergyCd - Intergranular Cracking
Cm - Kalling Etched Micrography by OMDf - Martensite, delta ferrite & carbides

ML00046 / Jan.2018
Brittle Fracture of SS Shear Pin
M - Martensitic Stainless SteelP - Machined PartAp - EnergyCd - Intergranular Cracking
Cm - Kalling Etched Micrography by OMDf - Martensite, delta ferrite & carbides