UNS

7 cases · 19 images

Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00176 / Nov.2021
Hydride Formation in a Titanium Blade
M - Unalloyed TitaniumP - BladeAp - Oil and GasCd - Hydride Formation
Cm - Surface Aspect by SEMDf - At the Surface
ML00170 / Sep.2020
MIC in Aluminum Brass Tubes
M - Aluminum BrassP - Seamless tubeAp - MaritimeCd - Preferential Dissolution
Cm - Surface Aspect by SEMDf - Internal Surface
ML00156 / Jan.2020
Antique Silver Plated Decorative Piece
M - BrassP - Decorative PieceAp - OrnamentalCd - Non Destructive Examination
Cm - Surface Aspect by SEMDf - At the Surface
ML00145 / Sep.2018
Impact of a .380 Winchester on 6061 T6 Plate
M - Aluminum Magnesium SiliconP - Rolled PlateAp - StructureCd - Pierced
Cm - Surface Aspect by SEMDf - At the Surface
ML00095 / Sep.2017
MIC of a Riser Control Line
M - Austenitic Stainless SteelP - Fabrication WeldAp - Oil and GasCd - Brittle Behavior
Cm - Surface Aspect by SEMDf - External Surface
ML00094 / Sep.2017
MIC of a Subsea Hydraulic Line
M - Super Duplex Stainless SteelP - Fabrication WeldAp - SubseaCd - Brittle Behavior
Cm - Surface Aspect by SEMDf - External Surface
ML00012 / Aug.2017
Vibration Induced Fatigue in a 316/316L SS
M - Austenitic Stainless SteelP - Seamless PipeAp - OffshoreCd - Vibration Induced Fatigue
Cm - Surface Aspect by SEMDf - External Surface

More from these cases

ML00156 — Antique Silver Plated Decorative PieceM - BrassP - Decorative PieceAp - OrnamentalCd - Non Destructive Examination
ML00156 / Jan.2020
Antique Silver Plated Decorative Piece
M - BrassP - Decorative PieceAp - OrnamentalCd - Non Destructive Examination
Cm - Surface Aspect by SEMDf - At the Surface
ML00156 / Jan.2020
Antique Silver Plated Decorative Piece
M - BrassP - Decorative PieceAp - OrnamentalCd - Non Destructive Examination
Cm - Surface Aspect by SEMDf - At the Surface
ML00156 / Jan.2020
Antique Silver Plated Decorative Piece
M - BrassP - Decorative PieceAp - OrnamentalCd - Non Destructive Examination
Cm - Surface Aspect by SEMDf - At the Surface
ML00145 — Impact of a .380 Winchester on 6061 T6 PlateM - Aluminum Magnesium SiliconP - Rolled PlateAp - StructureCd - Pierced
ML00145 / Sep.2018
Impact of a .380 Winchester on 6061 T6 Plate
M - Aluminum Magnesium SiliconP - Rolled PlateAp - StructureCd - Pierced
Cm - Surface Aspect by SEMDf - At the Surface
ML00145 / Sep.2018
Impact of a .380 Winchester on 6061 T6 Plate
M - Aluminum Magnesium SiliconP - Rolled PlateAp - StructureCd - Pierced
Cm - Surface Aspect by SEMDf - At the Surface
ML00145 / Sep.2018
Impact of a .380 Winchester on 6061 T6 Plate
M - Aluminum Magnesium SiliconP - Rolled PlateAp - StructureCd - Pierced
Cm - Surface Aspect by SEMDf - At the Surface
ML00095 — MIC of a Riser Control LineM - Austenitic Stainless SteelP - Fabrication WeldAp - Oil and GasCd - Brittle Behavior
ML00095 / Sep.2017
MIC of a Riser Control Line
M - Austenitic Stainless SteelP - Fabrication WeldAp - Oil and GasCd - Brittle Behavior
Cm - Surface Aspect by SEMDf - External Surface
ML00095 / Sep.2017
MIC of a Riser Control Line
M - Austenitic Stainless SteelP - Fabrication WeldAp - Oil and GasCd - Brittle Behavior
Cm - Surface Aspect by SEMDf - External Surface
ML00094 — MIC of a Subsea Hydraulic LineM - Super Duplex Stainless SteelP - Fabrication WeldAp - SubseaCd - Brittle Behavior
ML00094 / Sep.2017
MIC of a Subsea Hydraulic Line
M - Super Duplex Stainless SteelP - Fabrication WeldAp - SubseaCd - Brittle Behavior
Cm - Surface Aspect by SEMDf - External Surface
ML00094 / Sep.2017
MIC of a Subsea Hydraulic Line
M - Super Duplex Stainless SteelP - Fabrication WeldAp - SubseaCd - Brittle Behavior
Cm - Surface Aspect by SEMDf - Internal Surface
ML00094 / Sep.2017
MIC of a Subsea Hydraulic Line
M - Super Duplex Stainless SteelP - Fabrication WeldAp - SubseaCd - Brittle Behavior
Cm - Surface Aspect by SEMDf - Internal Surface
ML00094 / Sep.2017
MIC of a Subsea Hydraulic Line
M - Super Duplex Stainless SteelP - Fabrication WeldAp - SubseaCd - Brittle Behavior
Cm - Surface Aspect by SEMDf - Internal Surface