UNS

4 cases · 5 images

Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00066 / May.2017
GMAW Welded Joint in 9%Ni Alloy Steel
M - Nickel Alloy SteelP - Welded Testpiece for QualificationAp - PipelineCd - Welding
Cm - Identification drawingDf - Welded Joint
ML00055 / Apr.2017
CA6NM Blade Remanufactured by Welding
M - Martensitic Stainless SteelP - Remanufacture by WeldingAp - EnergyCd - Removed From Service
Cm - Identification drawingDf - Welded Joint
ML00045 / Aug.2017
Subsea Tubular F6NM Martensitic SS
M - Martensitic Stainless SteelP - Fabrication WeldAp - OffshoreCd - Welding
Cm - Identification drawingDf - Welded Joint
ML00069 / May.2017
Liquation Cracks in SAW of Low Carbon Steel
M - Low Carbon SteelP - Fabrication WeldAp - AutomotiveCd - Welding Defect
Cm - Identification drawingDf - Welded Joint

More from these cases

ML00045 — Subsea Tubular F6NM Martensitic SSM - Martensitic Stainless SteelP - Fabrication WeldAp - OffshoreCd - Welding
ML00045 / Aug.2017
Subsea Tubular F6NM Martensitic SS
M - Martensitic Stainless SteelP - Fabrication WeldAp - OffshoreCd - Welding
Cm - Identification drawingDf - Welded Joint