UNS

4 cases · 6 images

Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00170 / Sep.2020
MIC in Aluminum Brass Tubes
M - Aluminum BrassP - Seamless tubeAp - MaritimeCd - Preferential Dissolution
Cm - Aspect Before AnalysisDf - Internal Surface
Aspect "as received" of the seamless tube at the curved position, showing the longitudinal crack and corrosion products at the tube surface.
836
ML00165 / Jul.2020
SCC of Aluminum Bronze Heating Coil
M - Aluminum BronzeP - Seamless tubeAp - Oil and GasCd - Stress Corrosion
Cm - Aspect Before AnalysisDf - General View
The 2 1/2" nominal diameter seamless tube is externally cladded with stainless steel.
196
ML00056 / May.2018
Seamless Tube Externally Cladded with SS
M - Carbon Steel / Stainless SteelP - CladdingAp - Pulp and PaperCd - Removed From Service
Cm - Aspect Before AnalysisDf - Welded Joint
Seam welded tube, nominal diameter 2 1/4" and thickness 1/16".
106
ML00026 / Feb.2017
Autogenous Seam Welded Tube in Ferritic SS
M - Ferritic Stainless SteelP - Fabrication WeldAp - AutomotiveCd - Typical manufacturing
Cm - Aspect Before AnalysisDf - Autogenous Weld

More from these cases

ML00165 — SCC of Aluminum Bronze Heating CoilM - Aluminum BronzeP - Seamless tubeAp - Oil and GasCd - Stress Corrosion
ML00165 / Jul.2020
SCC of Aluminum Bronze Heating Coil
M - Aluminum BronzeP - Seamless tubeAp - Oil and GasCd - Stress Corrosion
Cm - Aspect Before AnalysisDf - General View
ML00165 / Jul.2020
SCC of Aluminum Bronze Heating Coil
M - Aluminum BronzeP - Seamless tubeAp - Oil and GasCd - Stress Corrosion
Cm - Aspect Before AnalysisDf - Internal Surface