UNS

7 cases · 7 images

Crevice Corrosion in a Subsea System — Aspect Before Analysis

View of the iinternal side of the tube (water side), deformed in the overheated area. There are several leaking points.
115
ML00180 / Mar.2022
Local Melting of Copper Cooling Tubes
M - Pure CopperP - Cooling TubeAp - SiderurgyCd - Overheating
Cm - Aspect Before AnalysisDf - Internal Surface
ML00170 / Sep.2020
MIC in Aluminum Brass Tubes
M - Aluminum BrassP - Seamless tubeAp - MaritimeCd - Preferential Dissolution
Cm - Aspect Before AnalysisDf - Internal Surface
ML00165 / Jul.2020
SCC of Aluminum Bronze Heating Coil
M - Aluminum BronzeP - Seamless tubeAp - Oil and GasCd - Stress Corrosion
Cm - Aspect Before AnalysisDf - Internal Surface
ML00155 / Jan.2020
Failure of a Prestressed Concrete Steel Strand
M - High Carbon SteelP - Wire RopeAp - StructureCd - Corrosion Fatigue
Cm - Aspect Before AnalysisDf - Internal Surface
ML00129 / Apr.2018
Non qualified WPS for High Strength Steel
M - Low Alloy Medium Carbon QTP - Welded Testpiece for QualificationAp - Oil and GasCd - Non qualified
Cm - Aspect Before AnalysisDf - Internal Surface
ML00094 / Sep.2017
MIC of a Subsea Hydraulic Line
M - Super Duplex Stainless SteelP - Fabrication WeldAp - SubseaCd - Brittle Behavior
Cm - Aspect Before AnalysisDf - Internal Surface
ML00012 / Aug.2017
Vibration Induced Fatigue in a 316/316L SS
M - Austenitic Stainless SteelP - Seamless PipeAp - OffshoreCd - Vibration Induced Fatigue
Cm - Aspect Before AnalysisDf - Internal Surface