Crevice Corrosion in a Subsea System — Aspect Before Analysis

Aspect of the 3 1/2" diameter tube after the water leakage in high temperature.
962
ML00180 / Mar.2022
Local Melting of Copper Cooling Tubes
M - Pure CopperP - Cooling TubeAp - SiderurgyCd - Overheating
Cm - Aspect Before AnalysisDf - General View

More from these cases

ML00180 — Local Melting of Copper Cooling TubesM - Pure CopperP - Cooling TubeAp - SiderurgyCd - Overheating
View of the iinternal side of the tube (water side), deformed in the overheated area. There are several leaking points.
115
ML00180 / Mar.2022
Local Melting of Copper Cooling Tubes
M - Pure CopperP - Cooling TubeAp - SiderurgyCd - Overheating
Cm - Aspect Before AnalysisDf - Internal Surface