B

4 cases · 12 images

Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00179 / Feb.2022
Hydrides in Titanium Weld
M - Unalloyed TitaniumP - In Field WeldAp - Chemical IndustryCd - Hydride Formation
Cm - Fractography by SEMDf - Fracture
ML00041 / Jun.2017
Fatigue Fracture of Inconel 718 Spline Shaft
M - NiCrFe AlloyP - ShaftAp - Oil and GasCd - Vibration Induced Fatigue
Cm - Fractography by SEMDf - Fatigue Fracture
After opening the crack the fracture surface presented different aspects close to the internal surface and through the wall propagation.  Intergranular at the surface, showing intergranular SCC mechanism, and transgranular with striation, showing the contribution of pulsing loads.
101
ML00011 / Oct.2017
Intergranular SCC of Pure Nickel
M - Unalloyed NickelP - Wrought FittingAp - Chemical IndustryCd - Stress Corrosion
Cm - Fractography by SEMDf - Through Wall Cracking
The fracture micromechanism is ductile for the pin that has been sheared in a condition of controlling the load carrying. Elongated Dimples.
453
ML00007 / Dec.2020
Free Machining Brass in Shear Pin
M - BrassP - Machined PartAp - LiftingCd - Shear
Cm - Fractography by SEMDf - Elongated Dimples

More from these cases

ML00179 — Hydrides in Titanium WeldM - Unalloyed TitaniumP - In Field WeldAp - Chemical IndustryCd - Hydride Formation
ML00179 / Feb.2022
Hydrides in Titanium Weld
M - Unalloyed TitaniumP - In Field WeldAp - Chemical IndustryCd - Hydride Formation
Cm - Fractography by SEMDf - Brittle Cracks
ML00179 / Feb.2022
Hydrides in Titanium Weld
M - Unalloyed TitaniumP - In Field WeldAp - Chemical IndustryCd - Hydride Formation
Cm - Fractography by SEMDf - Secondary Cracks
ML00179 / Feb.2022
Hydrides in Titanium Weld
M - Unalloyed TitaniumP - In Field WeldAp - Chemical IndustryCd - Hydride Formation
Cm - Fractography by SEMDf - Fatigue Striation
ML00041 — Fatigue Fracture of Inconel 718 Spline ShaftM - NiCrFe AlloyP - ShaftAp - Oil and GasCd - Vibration Induced Fatigue
ML00041 / Jun.2017
Fatigue Fracture of Inconel 718 Spline Shaft
M - NiCrFe AlloyP - ShaftAp - Oil and GasCd - Vibration Induced Fatigue
Cm - Fractography by SEMDf - Fatigue Fracture
ML00011 — Intergranular SCC of Pure NickelM - Unalloyed NickelP - Wrought FittingAp - Chemical IndustryCd - Stress Corrosion
ML00011 / Oct.2017
Intergranular SCC of Pure Nickel
M - Unalloyed NickelP - Wrought FittingAp - Chemical IndustryCd - Stress Corrosion
Cm - Fractography by SEMDf - Intergranular Cracking
ML00011 / Oct.2017
Intergranular SCC of Pure Nickel
M - Unalloyed NickelP - Wrought FittingAp - Chemical IndustryCd - Stress Corrosion
Cm - Fractography by SEMDf - Fatigue Striation
ML00011 / Oct.2017
Intergranular SCC of Pure Nickel
M - Unalloyed NickelP - Wrought FittingAp - Chemical IndustryCd - Stress Corrosion
Cm - Fractography by SEMDf - Fatigue Striation
ML00007 — Free Machining Brass in Shear PinM - BrassP - Machined PartAp - LiftingCd - Shear
ML00007 / Dec.2020
Free Machining Brass in Shear Pin
M - BrassP - Machined PartAp - LiftingCd - Shear
Cm - Fractography by SEMDf - Ductile Fracture