ASTM
10 cases · 38 images
Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00179 / Feb.2022
Hydrides in Titanium Weld
M - Unalloyed TitaniumP - In Field WeldAp - Chemical IndustryCd - Hydride Formation
Cm - Kroll Etched Micrography by OMDf - Weld Metal

ML00178 / Jan.2022
Cold cracks in Cr-Mo Welded Forging
M - CrMo SteelP - ForgingAp - O&G Well DrillingCd - Welding Defect
Cm - Nital Etched Micrography by OMDf - Weld Metal

ML00177 / Dec.2021
Cr-Mo Seam Welded Tube
M - CrMo SteelP - Longitudinally Seam WeldedAp - Fired HeaterCd - Not according to spec
Cm - Nital Etched Micrography by OMDf - Weld Metal in the Cap

ML00150 / Dec.2018
Vibration Induced Fatigue in a SS Oil Piping
M - Duplex Stainless SteelP - PipingAp - FPSOCd - Vibration Induced Fatigue
Cm - NaOH Electrolytic Etched MicroDf - Weld Metal

ML00065 / May.2017
Erosion Corrosion of Monel Piping
M - NiCu AlloyP - Seamless PipeAp - Chemical IndustryCd - Erosion Corrosion
Cm - Kalling Etched Micrography by OMDf - Weld Metal in the Root

ML00066 / May.2017
GMAW Welded Joint in 9%Ni Alloy Steel
M - Nickel Alloy SteelP - Welded Testpiece for QualificationAp - PipelineCd - Welding
Cm - Eletrolytically Etched Micrography by OMDf - Weld Metal in the Center

ML00055 / Apr.2017
CA6NM Blade Remanufactured by Welding
M - Martensitic Stainless SteelP - Remanufacture by WeldingAp - EnergyCd - Removed From Service
Cm - Kalling Etched Micrography by OMDf - Weld Metal

ML00045 / Aug.2017
Subsea Tubular F6NM Martensitic SS
M - Martensitic Stainless SteelP - Fabrication WeldAp - OffshoreCd - Welding
Cm - Kalling Etched Micrography by OMDf - Weld Metal
More from these cases

ML00179 / Feb.2022
Hydrides in Titanium Weld
M - Unalloyed TitaniumP - In Field WeldAp - Chemical IndustryCd - Hydride Formation
Cm - Kroll Etched Micrography by OMDf - Weld Metal

ML00179 / Feb.2022
Hydrides in Titanium Weld
M - Unalloyed TitaniumP - In Field WeldAp - Chemical IndustryCd - Hydride Formation
Cm - Kroll Etched Micrography by OMDf - Weld Metal
ML00179 / Feb.2022
Hydrides in Titanium Weld
M - Unalloyed TitaniumP - In Field WeldAp - Chemical IndustryCd - Hydride Formation
Cm - Micrography by OMDf - Weld Metal

ML00177 / Dec.2021
Cr-Mo Seam Welded Tube
M - CrMo SteelP - Longitudinally Seam WeldedAp - Fired HeaterCd - Not according to spec
Cm - Nital Etched Micrography by OMDf - Weld Metal in the Cap

ML00177 / Dec.2021
Cr-Mo Seam Welded Tube
M - CrMo SteelP - Longitudinally Seam WeldedAp - Fired HeaterCd - Not according to spec
Cm - Nital Etched Micrography by OMDf - Weld Metal in the Center

ML00177 / Dec.2021
Cr-Mo Seam Welded Tube
M - CrMo SteelP - Longitudinally Seam WeldedAp - Fired HeaterCd - Not according to spec
Cm - Nital Etched Micrography by OMDf - Weld Metal

ML00177 / Dec.2021
Cr-Mo Seam Welded Tube
M - CrMo SteelP - Longitudinally Seam WeldedAp - Fired HeaterCd - Not according to spec
Cm - Nital Etched Micrography by OMDf - Weld Metal in the Root

ML00177 / Dec.2021
Cr-Mo Seam Welded Tube
M - CrMo SteelP - Longitudinally Seam WeldedAp - Fired HeaterCd - Not according to spec
Cm - Nital Etched Micrography by OMDf - Weld Metal in the Root

ML00150 / Dec.2018
Vibration Induced Fatigue in a SS Oil Piping
M - Duplex Stainless SteelP - PipingAp - FPSOCd - Vibration Induced Fatigue
Cm - NaOH Electrolytic Etched MicroDf - Weld Metal

ML00150 / Dec.2018
Vibration Induced Fatigue in a SS Oil Piping
M - Duplex Stainless SteelP - PipingAp - FPSOCd - Vibration Induced Fatigue
Cm - NaOH Electrolytic Etched MicroDf - Weld Metal

ML00150 / Dec.2018
Vibration Induced Fatigue in a SS Oil Piping
M - Duplex Stainless SteelP - PipingAp - FPSOCd - Vibration Induced Fatigue
Cm - NaOH Electrolytic Etched MicroDf - Weld Metal

ML00065 / May.2017
Erosion Corrosion of Monel Piping
M - NiCu AlloyP - Seamless PipeAp - Chemical IndustryCd - Erosion Corrosion
Cm - Kalling Etched Micrography by OMDf - Weld Metal in the Root

ML00065 / May.2017
Erosion Corrosion of Monel Piping
M - NiCu AlloyP - Seamless PipeAp - Chemical IndustryCd - Erosion Corrosion
Cm - Kalling Etched Micrography by OMDf - Weld Metal in the Center

ML00065 / May.2017
Erosion Corrosion of Monel Piping
M - NiCu AlloyP - Seamless PipeAp - Chemical IndustryCd - Erosion Corrosion
Cm - Kalling Etched Micrography by OMDf - Weld Metal in the Center

ML00065 / May.2017
Erosion Corrosion of Monel Piping
M - NiCu AlloyP - Seamless PipeAp - Chemical IndustryCd - Erosion Corrosion
Cm - Kalling Etched Micrography by OMDf - Weld Metal in the Cap

ML00065 / May.2017
Erosion Corrosion of Monel Piping
M - NiCu AlloyP - Seamless PipeAp - Chemical IndustryCd - Erosion Corrosion
Cm - Kalling Etched Micrography by OMDf - Weld Metal in the Cap

ML00066 / May.2017
GMAW Welded Joint in 9%Ni Alloy Steel
M - Nickel Alloy SteelP - Welded Testpiece for QualificationAp - PipelineCd - Welding
Cm - Eletrolytically Etched Micrography by OMDf - Weld Metal in the Center

ML00066 / May.2017
GMAW Welded Joint in 9%Ni Alloy Steel
M - Nickel Alloy SteelP - Welded Testpiece for QualificationAp - PipelineCd - Welding
Cm - Eletrolytically Etched Micrography by OMDf - Weld Metal in the Cap

ML00066 / May.2017
GMAW Welded Joint in 9%Ni Alloy Steel
M - Nickel Alloy SteelP - Welded Testpiece for QualificationAp - PipelineCd - Welding
Cm - Eletrolytically Etched Micrography by OMDf - Weld Metal in the Cap

ML00055 / Apr.2017
CA6NM Blade Remanufactured by Welding
M - Martensitic Stainless SteelP - Remanufacture by WeldingAp - EnergyCd - Removed From Service
Cm - Kalling Etched Micrography by OMDf - Weld Metal

ML00045 / Aug.2017
Subsea Tubular F6NM Martensitic SS
M - Martensitic Stainless SteelP - Fabrication WeldAp - OffshoreCd - Welding
Cm - Kalling Etched Micrography by OMDf - Weld Metal in the Center

ML00045 / Aug.2017
Subsea Tubular F6NM Martensitic SS
M - Martensitic Stainless SteelP - Fabrication WeldAp - OffshoreCd - Welding
Cm - Kalling Etched Micrography by OMDf - Weld Metal

ML00045 / Aug.2017
Subsea Tubular F6NM Martensitic SS
M - Martensitic Stainless SteelP - Fabrication WeldAp - OffshoreCd - Welding
Cm - Kalling Etched Micrography by OMDf - Weld Metal in the Root

ML00045 / Aug.2017
Subsea Tubular F6NM Martensitic SS
M - Martensitic Stainless SteelP - Fabrication WeldAp - OffshoreCd - Welding
Cm - Kalling Etched Micrography by OMDf - Weld Metal in the Center

ML00045 / Aug.2017
Subsea Tubular F6NM Martensitic SS
M - Martensitic Stainless SteelP - Fabrication WeldAp - OffshoreCd - Welding
Cm - Kalling Etched Micrography by OMDf - Weld Metal in the Center