ASTM
3 cases · 7 images
Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00123 / Feb.2018
Non Qualified Superduplex for Subsea
M - Super Duplex Stainless SteelP - BarAp - Oil and GasCd - Not according to spec
Cm - Fractography by SEMDf - Broken Testpiece

ML00041 / Jun.2017
Fatigue Fracture of Inconel 718 Spline Shaft
M - NiCrFe AlloyP - ShaftAp - Oil and GasCd - Vibration Induced Fatigue
Cm - Fractography by SEMDf - Fatigue Fracture

ML00007 / Dec.2020
Free Machining Brass in Shear Pin
M - BrassP - Machined PartAp - LiftingCd - Shear
Cm - Fractography by SEMDf - Elongated Dimples
More from these cases

ML00123 / Feb.2018
Non Qualified Superduplex for Subsea
M - Super Duplex Stainless SteelP - BarAp - Oil and GasCd - Not according to spec
Cm - Fractography by SEMDf - Broken Testpiece

ML00123 / Feb.2018
Non Qualified Superduplex for Subsea
M - Super Duplex Stainless SteelP - BarAp - Oil and GasCd - Not according to spec
Cm - Fractography by SEMDf - Broken Testpiece

ML00041 / Jun.2017
Fatigue Fracture of Inconel 718 Spline Shaft
M - NiCrFe AlloyP - ShaftAp - Oil and GasCd - Vibration Induced Fatigue
Cm - Fractography by SEMDf - Fatigue Fracture

ML00007 / Dec.2020
Free Machining Brass in Shear Pin
M - BrassP - Machined PartAp - LiftingCd - Shear
Cm - Fractography by SEMDf - Ductile Fracture