ASTM

20 cases · 70 images

Crevice Corrosion in a Subsea System — Aspect Before Analysis

ASTM — sub-branches

ML00134 / Aug.2020
Brittle Fracture of a Superduplex Valve Body
M - Super Duplex Stainless SteelP - Fabrication WeldAp - SubseaCd - Brittle Fracture
Cm - Fractography by SEMDf - Cleavage Facets
Aspect of the bolt fracture surface by scanning electron microscopy, (SEM) presenting striations that indicate a FATIGUE micromechanism.  The bolt is of a medium strength (class 8.8) low alloy steel, medium carbon, quenched and tempered.
1123
ML00130 / Jun.2018
Fatigue Fracture of Overloaded Bolts
M - Low Alloy Medium Carbon QTP - FastenerAp - O&G Well DrillingCd - Mechanical Fatigue
Cm - Fractography by SEMDf - Fatigue Fracture
Fractographic detail of the longitudinal Charpy V testpiece,  broken at -46°C and presenting energy of 64J (the average energy of three tespieces was 70J).  The Charpy V testpiece was removed from the center of the bar. The micromechanism is quasicleavage and the test in this direction presented energy values superior than the minimum requirement of 45J.
945
ML00123 / Feb.2018
Non Qualified Superduplex for Subsea
M - Super Duplex Stainless SteelP - BarAp - Oil and GasCd - Not according to spec
Cm - Fractography by SEMDf - Broken Testpiece
The hose connector fracture surface presented different fracture micromechanisms associated to the microstructure: inclusion decohesion, small regions of intergranular fractures (probably due to cementite at grain boundaries), and cleavage of the ferritic structure.  All these mechanisms are brittle.
560
ML00103 / Nov.2017
Brittle Fracture of a Free-Cutting Connector
M - Low Carbon SteelP - Machined PartAp - ShipCd - Brittle Fracture
Cm - Fractography by SEMDf - Brittle Fracture
ML00071 / Jan.2019
Reheating Cracking of a CrMo Vessel Weld
M - CrMo SteelP - In Field WeldAp - EnergyCd - Welding Defect
Cm - Fractography by SEMDf - Fracture
Fracture surface after opening the shell cracking, presenting fatigue striation.  The fracture presents also foreign particles.
132
ML00050 / Nov.2017
Fatigue Failure of a 316SS Pressure Stabilizer
M - Austenitic Stainless SteelP - Fabrication WeldAp - Chemical IndustryCd - Mechanical Fatigue
Cm - Fractography by SEMDf - Fatigue Striation
ML00041 / Jun.2017
Fatigue Fracture of Inconel 718 Spline Shaft
M - NiCrFe AlloyP - ShaftAp - Oil and GasCd - Vibration Induced Fatigue
Cm - Fractography by SEMDf - Fatigue Fracture
The fracture surface is flat, shows the graphite nodules and cleavage of the ferritic microstructure, indicating that the material have exceeded the capacity to acomodate the stress.
945
ML00040 / Apr.2017
Brittle Fracture of a Valve Stem
M - Nodular Cast IronP - Valve StemAp - ShipCd - Brittle Fracture
Cm - Fractography by SEMDf - Cleavage Facets

More from these cases

ML00134 — Brittle Fracture of a Superduplex Valve BodyM - Super Duplex Stainless SteelP - Fabrication WeldAp - SubseaCd - Brittle Fracture
ML00134 / Aug.2020
Brittle Fracture of a Superduplex Valve Body
M - Super Duplex Stainless SteelP - Fabrication WeldAp - SubseaCd - Brittle Fracture
Cm - Fractography by SEMDf - Cleavage Facets
ML00134 / Aug.2020
Brittle Fracture of a Superduplex Valve Body
M - Super Duplex Stainless SteelP - Fabrication WeldAp - SubseaCd - Brittle Fracture
Cm - Fractography by SEMDf - Secondary Cracks
ML00130 — Fatigue Fracture of Overloaded BoltsM - Low Alloy Medium Carbon QTP - FastenerAp - O&G Well DrillingCd - Mechanical Fatigue
Aspect of the fracture surface in low magnification, showing a flat aspect (associated to a fatigue fracture micromechanims) and a rough aspect (associated to a ductile fracture micromechanism).
167
ML00130 / Jun.2018
Fatigue Fracture of Overloaded Bolts
M - Low Alloy Medium Carbon QTP - FastenerAp - O&G Well DrillingCd - Mechanical Fatigue
Cm - Fractography by SEMDf - General View
Aspect of the fracture surface by scanning electron microscopy, presenting fatigue striations micromechanism.  The bolt is a medium strength low alloy steel, medium carbon, quenched and tempered.
154
ML00130 / Jun.2018
Fatigue Fracture of Overloaded Bolts
M - Low Alloy Medium Carbon QTP - FastenerAp - O&G Well DrillingCd - Mechanical Fatigue
Cm - Fractography by SEMDf - Fatigue Fracture
Detailed fractographic aspect of the flat part of the bolt fracture, presenting fatigue striations.  The bolt is a medium strength low alloy steel, medium carbon, quenched and tempered.
141
ML00130 / Jun.2018
Fatigue Fracture of Overloaded Bolts
M - Low Alloy Medium Carbon QTP - FastenerAp - O&G Well DrillingCd - Mechanical Fatigue
Cm - Fractography by SEMDf - Fatigue Fracture
Fractographic detailed aspect of the rough part of the fracture surface, presenting ductile dimples.  This is the final fracture, by overload.
137
ML00130 / Jun.2018
Fatigue Fracture of Overloaded Bolts
M - Low Alloy Medium Carbon QTP - FastenerAp - O&G Well DrillingCd - Mechanical Fatigue
Cm - Fractography by SEMDf - Ductile Fracture
ML00123 — Non Qualified Superduplex for SubseaM - Super Duplex Stainless SteelP - BarAp - Oil and GasCd - Not according to spec
Fractography of the broken Charpy V testpiece,  longitudinal, broken at -46°C and presenting energy of 64J (the average of three values was 70J).  In this direction the material presented an energy value higher than the minimum requirement of 45J.
109
ML00123 / Feb.2018
Non Qualified Superduplex for Subsea
M - Super Duplex Stainless SteelP - BarAp - Oil and GasCd - Not according to spec
Cm - Fractography by SEMDf - Broken Testpiece
Fractography of the Charpy V testpiece, transverse section, broken at -46°C and presenting energy of 20J (the average of three results was 33J).  The coarse structure and the alignement created a condition for low energy results in this specific direction, and the material did not present the minimum requirement of 45J.
103
ML00123 / Feb.2018
Non Qualified Superduplex for Subsea
M - Super Duplex Stainless SteelP - BarAp - Oil and GasCd - Not according to spec
Cm - Fractography by SEMDf - Broken Testpiece
ML00103 — Brittle Fracture of a Free-Cutting ConnectorM - Low Carbon SteelP - Machined PartAp - ShipCd - Brittle Fracture
ML00103 / Nov.2017
Brittle Fracture of a Free-Cutting Connector
M - Low Carbon SteelP - Machined PartAp - ShipCd - Brittle Fracture
Cm - Fractography by SEMDf - Cleavage Facets
ML00103 / Nov.2017
Brittle Fracture of a Free-Cutting Connector
M - Low Carbon SteelP - Machined PartAp - ShipCd - Brittle Fracture
Cm - Fractography by SEMDf - Brittle Fracture
ML00103 / Nov.2017
Brittle Fracture of a Free-Cutting Connector
M - Low Carbon SteelP - Machined PartAp - ShipCd - Brittle Fracture
Cm - Fractography by SEMDf - Intergranular Fracture
ML00071 — Reheating Cracking of a CrMo Vessel WeldM - CrMo SteelP - In Field WeldAp - EnergyCd - Welding Defect
ML00071 / Jan.2019
Reheating Cracking of a CrMo Vessel Weld
M - CrMo SteelP - In Field WeldAp - EnergyCd - Welding Defect
Cm - Fractography by SEMDf - Intergranular Cracking
ML00041 — Fatigue Fracture of Inconel 718 Spline ShaftM - NiCrFe AlloyP - ShaftAp - Oil and GasCd - Vibration Induced Fatigue
ML00041 / Jun.2017
Fatigue Fracture of Inconel 718 Spline Shaft
M - NiCrFe AlloyP - ShaftAp - Oil and GasCd - Vibration Induced Fatigue
Cm - Fractography by SEMDf - Fatigue Fracture
ML00040 — Brittle Fracture of a Valve StemM - Nodular Cast IronP - Valve StemAp - ShipCd - Brittle Fracture
Detail of the cleavage micromechanism.
195
ML00040 / Apr.2017
Brittle Fracture of a Valve Stem
M - Nodular Cast IronP - Valve StemAp - ShipCd - Brittle Fracture
Cm - Fractography by SEMDf - Cleavage Facets