Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00147 / Aug.2018
WC Layer Detached from a Cast Lean Duplex
M - Lean Duplex Stainless SteelP - Centrifugal CastingAp - ShipCd - Lack of Sealing
Cm - Electrolytic Etch Micrography by SEMDf - Thermal Spray Layer

ML00137 / Mar.2021
Brittle Fracture of a 15-5 PH Valve Spring
M - Precipitation Hardened Stainless SteelP - SpringAp - Oil and GasCd - Brittle Behavior
Cm - Surface Aspect by SEMDf - Corrosion
More from these cases

ML00147 / Aug.2018
WC Layer Detached from a Cast Lean Duplex
M - Lean Duplex Stainless SteelP - Centrifugal CastingAp - ShipCd - Lack of Sealing
Cm - Electrolytic Etch Micrography by SEMDf - Thermal Spray Layer

ML00147 / Aug.2018
WC Layer Detached from a Cast Lean Duplex
M - Lean Duplex Stainless SteelP - Centrifugal CastingAp - ShipCd - Lack of Sealing
Cm - Electrolytic Etch Micrography by SEMDf - Sigma

ML00137 / Mar.2021
Brittle Fracture of a 15-5 PH Valve Spring
M - Precipitation Hardened Stainless SteelP - SpringAp - Oil and GasCd - Brittle Behavior
Cm - Surface Aspect by SEMDf - Corrosion

ML00137 / Mar.2021
Brittle Fracture of a 15-5 PH Valve Spring
M - Precipitation Hardened Stainless SteelP - SpringAp - Oil and GasCd - Brittle Behavior
Cm - Fractography by SEMDf - At the Surface

ML00137 / Mar.2021
Brittle Fracture of a 15-5 PH Valve Spring
M - Precipitation Hardened Stainless SteelP - SpringAp - Oil and GasCd - Brittle Behavior
Cm - Fractography by SEMDf - Intergranular Fracture

ML00137 / Mar.2021
Brittle Fracture of a 15-5 PH Valve Spring
M - Precipitation Hardened Stainless SteelP - SpringAp - Oil and GasCd - Brittle Behavior
Cm - Fractography by SEMDf - Intergranular Fracture

ML00137 / Mar.2021
Brittle Fracture of a 15-5 PH Valve Spring
M - Precipitation Hardened Stainless SteelP - SpringAp - Oil and GasCd - Brittle Behavior
Cm - Fractography by SEMDf - Fracture