81
VIEW
ML00071 / Jan.2019
Reheating Cracking of a CrMo Vessel Weld
M
- CrMo Steel
P
- In Field Weld
Ap
- Energy
Cd
- Welding Defect
Cm
- Transverse Section Aspect
Df
- Weld Metal