A
1 case · 2 images
Crevice Corrosion in a Subsea System — Aspect Before Analysis
Condition: Casting Defect ×Capture method: Optical Microscope ×Detail focus: Non Metallic Inclusions ×clear all
A — sub-branches

ML00017 / Apr.2017
Casting Defect in CA6NM
M - Martensitic Stainless SteelP - Machined PartAp - EnergyCd - Casting Defect
Cm - Micrography by OMDf - Non Metallic Inclusions
More from these cases

ML00017 / Apr.2017
Casting Defect in CA6NM
M - Martensitic Stainless SteelP - Machined PartAp - EnergyCd - Casting Defect
Cm - Kalling Etched Micrography by OMDf - Non Metallic Inclusions