A
1 case · 1 image
Crevice Corrosion in a Subsea System — Aspect Before Analysis
Atlas
/
Standard
/
ASTM
/ A
Condition: Welding Defect
×
Capture method: Fracture Surface Aspect
×
clear all
A — sub-branches
182
1
234
1
335
1
36
1
514
1
515
1
Results
Sort
Newest
Oldest
Title A-Z
Title Z-A
61
VIEW
ML00010 / Oct.2017
Cold Cracks in a Gouged Weld Metal
M
- Low Alloy Low Carbon QT
P
- Rolled Plate
Ap
- Offshore
Cd
- Welding Defect
Cm
- Fracture Surface Aspect
Df
- Fish Eye